SOLUBILITY CHARACTERISTICS OF GaAs IN Bi AND THEIR PHASE DIAGRAM
FENG Shuifu;ZHOU Jicheng Shanghai Institute of Metallurgy; Academia Sinica Shanghai Institute of Metallurgy;Academia Sinica;Shanghai 200050
Cite this article: 

FENG Shuifu;ZHOU Jicheng Shanghai Institute of Metallurgy; Academia Sinica Shanghai Institute of Metallurgy;Academia Sinica;Shanghai 200050. SOLUBILITY CHARACTERISTICS OF GaAs IN Bi AND THEIR PHASE DIAGRAM. Acta Metall Sin, 1990, 26(2): 102-105.

Download:  PDF(386KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A modified liquid phase epitaxy apparatus for semiconductor materialswas used to measure the solubility of GaAs in Bi. The solubility of GaAs in Biand two phase diagrams rich in Bi under H_2 and N_2 atmosphere were obtained. Anew phenomenon, in which the parameters Q value (quantity of GaAs dissolved inBi in fixed time but various temperatures/saturated quantity of GaAs in Bi) weredifferent from each other and there existed a maximum Q value in particular tem-perature, was observed. This phenomenon can be recognized as a common feature ofa simple binary metallic system which has the phase diagram similar to that of Bi-GaAs. The difference observed from the dependence of Q values on temperature inboth H_2 and N_2 atmosphere was discussed.
Key words:  liquid phase epitaxy      solubility      phase diagram     
Received:  18 February 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I2/102

1 Rubenstein M. J Electrochem Soc, 1966; 113: 752
2 Hall R N. J Electrochem Soc, 1963; 110: 385
3 #12
4 冯水富,中国科学院上海冶金研究所硕士学位论文,1988
[1] ZHANG Lili, JI Zongwei, ZHAO Jiuzhou, HE Jie, JIANG Hongxiang. Key Factors Influencing Eutectic Si Modification in Al-Si Hypoeutectic Alloy by Trace La[J]. 金属学报, 2023, 59(11): 1541-1546.
[2] LI Yuxing, LIU Xinghao, WANG Cailin, HU Qihui, WANG Jinghan, MA Hongtao, ZHANG Nan. Research Progress on Corrosion Behavior of Gaseous CO2 Transportation Pipelines Containing Impurities[J]. 金属学报, 2021, 57(3): 283-294.
[3] GAO Xiang, ZHANG Guikai, XIANG Xin, LUO Lizhu, WANG Xiaolin. Effects of Alloying Elements on the Adsorption of Oxygen on V(110) Surfaces: A First-Principles Study[J]. 金属学报, 2020, 56(6): 919-928.
[4] Rongyao MA, Lin ZHAO, Changgang WANG, Xin MU, Xin WEI, Junhua DONG, Wei KE. Influence of Hydrostatic Pressure on the Thermodynamics and Kinetics of Metal Corrosion[J]. 金属学报, 2019, 55(2): 281-290.
[5] Zhibin FAN, Xiaoping LIN, Yun DONG, Jie YE, Chan LI, Bo LI. AGE-HARDENING RESPONSE FOR Mg96.17Zn3.15Y0.5Zr0.18 SOLID SOLUTION ALLOY UNDER HIGH PRESSURE[J]. 金属学报, 2016, 52(12): 1491-1496.
[6] ZHANG Weibin SHA Chunsheng DU Yong WEN Guanghua XIE Wen WANG Shequan. COMPUTER SIMULATIONS AND VERIFICATION OF GRADIENT ZONE FORMATION IN CEMENTED CARBIDES[J]. 金属学报, 2011, 47(10): 1307-1314.
[7] . A Model for Calculating Solubility of Hydrogen in Molten Alloys[J]. 金属学报, 2008, 44(2): 129-133 .
[8] Hua-Wei ZHANG. Hydrogen Solubility in Pure Metals for Gasar Process[J]. 金属学报, 2007, 43(2): 113-118 .
[9] ZHANG Huawei; LI Yanxiang; LIU Yuan. Study of Metal--Hydrogen Binary Phase Diagram in Gasar Process[J]. 金属学报, 2005, 41(1): 55-.
[10] ZHANG Jian(Metallurgical Engineering School; University of Science and Technology Beijing; Beijing 100083). CONSISTENCY(OR SIMILARITY) OF THERMODYNAMIC PROPERTIES OF METALLURGICAL MELTS WITH THEIR PHASE DIAGRAMS[J]. 金属学报, 1998, 34(7): 742-752.
[11] Zhang Jian (Institute of Metallurgy; University of Science and Technology Beijing; Beijing 100083). CLASSIFICATION OF THERMODYNAMIC PROPERTIES OF BINARY METALLIC MELTS ACCORDING TO THEIR PHASE DIAGRAMS[J]. 金属学报, 1998, 34(1): 75-85.
[12] LIU Gang;CHEN Ruiliang;LI Chonghe;CHEN Nianyi(Shanghai Institute of MetaIlurgy; Chinese Academy of Sciences; Shanghai 200050). REGULARITIES OF MUTUAL SOLUBILITY OF MOLTEN SALT-LIQUID METAL SYSTEMS[J]. 金属学报, 1997, 33(9): 939-942.
[13] ZHOU Hong; WANG Jinguo; JIA Shusheng (Jilin University of Technology; Chanerhun 130025) OGIKeisaku(Kyushu Universily; Japan) (Manuscript received 1996-03-22; in revised form 1997-04- 13). SOLIDIFIED MICROSTRUCTURES AND PHASES OF HIGH SPEED STEELS CONTA1NING DIFFERENT V AND C CONTENT[J]. 金属学报, 1997, 33(8): 838-843.
[14] FANG Jianhui; TANG Yun; LI Yu; YAN Licheng; CHEN Nianyi (Shanghai University;Shanghai 201800); WANG Jiyang (Shandong University; Jinan 250012)(Manuscript received 1996-04-08; in revised form 1996-09-10). KPO_3-M0O_3 PHASE DIAGRAM[J]. 金属学报, 1997, 33(4): 395-397.
[15] ZHOU Guozhi(Kuo-Chih Chou) (University of Science and Technology Beijing;Beiing 100083). NEW GENERATION SOLUTION GEOMETRICAL MODEL AND ITS FURTHER DEVELOPMENT[J]. 金属学报, 1997, 33(2): 126-132.
No Suggested Reading articles found!