GRAIN COARSENING TEMPERATURE OF V-Ti-N MICROALLOYING STEELS
TANG Guoyi;ZHENG Yangzeng;CAI Qigong;ZHU Jing Yanshan University; Qinhuangdao; Hebei Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing TANG Guoyi; Department of Graduates; Central Iron and Steel Research Institute Ministry of Metallurgical Industry; Beijing 100081
Cite this article: 

TANG Guoyi;ZHENG Yangzeng;CAI Qigong;ZHU Jing Yanshan University; Qinhuangdao; Hebei Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing TANG Guoyi; Department of Graduates; Central Iron and Steel Research Institute Ministry of Metallurgical Industry; Beijing 100081. GRAIN COARSENING TEMPERATURE OF V-Ti-N MICROALLOYING STEELS. Acta Metall Sin, 1989, 25(6): 30-36.

Download:  PDF(1054KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effects of chemical composition and cooling rate after solidifi-cation on the grain coarsening temperature, T_(GC), of the V-Ti-N microalloying steelshave been investigated. It is shown that the T_(GC) may be obviously raised byadding even a little Ti to the base steels so as to precipitate a great deal of fineTi-bearing grains of about 10 nm. The T_(GC) does not increase with the cooling rate,as it is over a certain critical value. The T_(GC) is insensitive to any variation ofN content at simulated cooling condition of 150mm continuouscast slab. TheT_(GC) may be dropped down about 100℃ by adding 0.33 wt-% Mo to the steels.The sensitivity of T_(GC) to cooling condition is related with Ti and N contents.
Key words:  microalloying steel      grain coarsening temperature      cooling rate after solidification     
Received:  18 June 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I6/30

1 唐国翌.东北重型机械学院硕士论文,1986
2 郑炀曾.唐国翌.物理测试,1986;(2) :54
3 徐祖耀.金属材料热力学,北京:科学出版社,1981:242
4 Carlsson J-E, Roberts W, Sandberg A. Swedish Institute for Metals Research Report, № 1438, 1980: 5
5 笠松裕,高嶋修嗣,细谷隆司.R&D神户制钢技报,1979;29(4) :53
6 Matsuda S, Okumura N. Trans Iron Steel Inst Jpn, 1978; 18: 198
7 George T J, Kennon N F. J Aust Inst Met, 1972; 17: 73
8 Hillert M. Acta Metall, 1965; 13: 227
No related articles found!
No Suggested Reading articles found!