TEMPERATURE DEPENDENCE OF CHANGE OF BORIDE IN Fe_(70)Cr_(18)Mo_2 SiB_9
LIN Yijian;HU Jian;YOU Yunlong;JING Chunyong;YU Quanqin Shanghai Iron and Steel Research Institute LIN Yijian;Measuring and Testing Centre; Shanghai Iron and Steel Research Institute; Shanghai 200940
Cite this article: 

LIN Yijian;HU Jian;YOU Yunlong;JING Chunyong;YU Quanqin Shanghai Iron and Steel Research Institute LIN Yijian;Measuring and Testing Centre; Shanghai Iron and Steel Research Institute; Shanghai 200940. TEMPERATURE DEPENDENCE OF CHANGE OF BORIDE IN Fe_(70)Cr_(18)Mo_2 SiB_9. Acta Metall Sin, 1989, 25(6): 120-125.

Download:  PDF(924KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The formation of borides M_2B, M_3B_2 and M_(23)B_6 may be carried outfrom the melt-quenched Fe_(70)Cr_(18)Mo_2SiB_9 during 700-1150℃ annealing. As the tem-perature raising, the M_2B, the majority being Fe_2B, may be gradually replaced byCr_2B via the co-existence between Fe_2B and Cr_2B. The Cr_2B may be formed by transformation of Fe_2B through the atomic substitution and structural adjustment. Thethin slice of remaining Fe_2B is sandwiched between (100) faces of (Cr,Fe)_2B asstacking fault. The M_3B_2 is virtually composed of the Mo_(1+x)(Fe,Cr)_(2-x)B_2 where x(0≤x≤1) increases with the increase of temperature.
Key words:  FeCrMoSiB alloy      M_2B      M_3B_2      M_(23)B_6     
Received:  18 June 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I6/120

1 林一坚,尤云龙,井春永,郁泉琴.钢铁研究学报,待发表
2 林一坚,尤云龙,张小岷,井春永,严守平,章靖国.金属学报,1987;23:A 346
3 Koester U, Heroid U, Krense D. In: Kear B H, Giessen B C, Cohen M eds., Rapidly Solidified Amorphous and Crystalline Alloys, New York: Elsevier Science, 1982: 179
4 Holt R T, Wallace W. Int Metall Rev, 1976; 21: 1
5 李玉清, 刘锦岩.理化检验(物理分册),1985;21:3
6 Pradelli G, Gianoglio C. Met Ital, 1976; 68: 591
7 Brown B E, Beerntsen D J. Acta Crystallogr. 1964; 17: 448
8 Roland Kiessling. Acta Chem Scand, 1950; 4: 146
No related articles found!
No Suggested Reading articles found!