Acta Metall Sin  1989, Vol. 25 Issue (5): 89-98    DOI:
Current Issue | Archive | Adv Search |
APPLICATION OF TRIANGLE MAPKOB CHAIN TO GRAVITY CONCENTRATION
WANG Weixing;HUANG Shu;CHBN Jin Central South University of Technology; Changsha WANG Weixing; Department of Mineral Engineering; Central South University ofTechnology; Changsha 410083
Cite this article: 

WANG Weixing;HUANG Shu;CHBN Jin Central South University of Technology; Changsha WANG Weixing; Department of Mineral Engineering; Central South University ofTechnology; Changsha 410083. APPLICATION OF TRIANGLE MAPKOB CHAIN TO GRAVITY CONCENTRATION. Acta Metall Sin, 1989, 25(5): 89-98.

Download:  PDF(731KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A mathematical model of flow-film type's gravity concentrators is be-ing developed based on the transfer probabilities of mineral particles, which are de-termined from the combination of the Bagnold's shearing theory with the principlesof Mapков processes. This model can be used to predict the grade, recovery andothers of the concentrate in terms of the feed and operating conditions.
Key words:  gravity concentration      mineral processing model      stochastic process      Марков process      sediment transport     
Received:  18 May 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I5/89

1 Einstein H A. The Bed-Load Function for Sediment Transportation in Open Channel Flows, Technical Bullentin 1026, USDA Soil Conservation Service, 1950
2 复旦大学.概率论(第三册),高等教育出版社,1981:34--60
3 武汉水电学院.河流泥沙工程学,水利出版社,1981:105
4 Bagnold R A. Proc R Soc London, Ser. A, 1954; 225: 49--63
5 浙江大学.概率论与数理统计,人民教育出版社,1979:54--65
6 Кузнедов Д С著,林鸿荪译.流体动力学,高等教育出版社,1955:105--107
7 Левич В Г著,戴干策,陈敏恒译.物理-化学流体动力学,上海科学技术出版社,1965:510--515
8 韩其为,何明民.泥沙运动统计理论,科学出版社,1984
9 王卫星,唐玉白,黄枢.有色金属,1986;38(1) :44--51
10 Wang Weixing (王卫星), Huang Shu (黄枢), Chen Jin (陈荩). International Symposium on the Production and Processing of Fine Particles, Saite-Foy, Canada, 198
[1] ZHOU Binghai ZHAI Ziqing. STOCHASTIC PROCESS-BASED MODELING METHOD FOR PITTING CORRSION OF Ni-BASED ALLOY 690[J]. 金属学报, 2011, 47(9): 1159-1166.
[2] WEI Dezhou;SUN Yubo Northeast University of Technology; Shenyang WEI Dezhou;lecturer;Department of Mineral Engineering;Northeast University of Techhnology;110006 Shenyang. APPLICABILITY OF SIMILITUDE PRINCIPLE TO STUDY STRATIFICATION THEORY OF GRAVITY CONCENTRATION[J]. 金属学报, 1989, 25(5): 99-106.
No Suggested Reading articles found!