Please wait a minute...
Acta Metall Sin  1989, Vol. 25 Issue (3): 146-148    DOI:
Current Issue | Archive | Adv Search |
ELECTRON ENEGRY SPECTRUM ANALYSIS FOR PASSIVATING FILM OF Si-BEARING STAINLESS STEELS
FENG Xiuying;QIN Zirui;LI Longsheng;SHENG Shishan;LIU Dejing Dolian University of Technology Dalian Institute of Chemical Physics; Academia Sinica Dalian Anti-acid Pump Factory
Cite this article: 

FENG Xiuying;QIN Zirui;LI Longsheng;SHENG Shishan;LIU Dejing Dolian University of Technology Dalian Institute of Chemical Physics; Academia Sinica Dalian Anti-acid Pump Factory. ELECTRON ENEGRY SPECTRUM ANALYSIS FOR PASSIVATING FILM OF Si-BEARING STAINLESS STEELS. Acta Metall Sin, 1989, 25(3): 146-148.

Download:  PDF(278KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The surface film on Si-bearing stainless steels formed aftersoaking in concentratednitric acid for 216h was investigated by means of electron energy spectrum analysis. It canbe reached from this investigation that Si builds up in the surface film in the form of silica.It plays as a main passivating element in Si-bearing stainless steels in strong oxidizing medium,whereas Cr drops into the second place.
Key words:  Si-bearing stainless steels      passivating film     
Received:  18 March 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I3/146

1 冶金工业部钢铁研究总院,兰州化学工业公司化工机械研究所.新金属材料,1977;(6) :1--6
2 冯秀英,李隆盛,刘德经,马安圣.大连工学院学报,1986;(4) :63
3 藤原和雄.铁钢,1985;71:795
4 李隆盛,秦紫瑞,冯秀英,刘德经.大连工学院学报,1981;(4) :47
5 Davis L E, MacDonald N C. Palmberg P W, Riach G E, Weber R E. Handbook of Auger Electron Spectroscopy. Minnesota: Physical Electronics Industries, 1976
6 王迅.材料保护,1982;(3) :5
7 Wagner C D. Handbook of X-Ray Photoelectron Spectroscopy, Minnesota: Physcial Electronics Industries, 1979
8 麻启承,傅守默,邹懿珠.见:麻启承主编,金属材料及热处理,北京:化学工业出版社,1980:152G
[1] XU Shumin;LENG Daguang (Zhaoyuan JINBAO Electronics Co.Ltd;Zhaoyuan 265400). A NEW TECHNOLOGY OF OXIDATION RESISTANCE OF COPPER FOIL[J]. 金属学报, 1998, 34(11): 1230-1232.