Please wait a minute...
Acta Metall Sin  1989, Vol. 25 Issue (2): 34-39    DOI:
Current Issue | Archive | Adv Search |
TEMPERED BAINITE EMBRITTLEMENT IN SOME STRUCTURAL STEELS
HU Guangli;LIU Zhengtang;WANG Ping;HUA Wenjun;KANG Mokuang Northwestern Polytechnical University
Cite this article: 

HU Guangli;LIU Zhengtang;WANG Ping;HUA Wenjun;KANG Mokuang Northwestern Polytechnical University. TEMPERED BAINITE EMBRITTLEMENT IN SOME STRUCTURAL STEELS. Acta Metall Sin, 1989, 25(2): 34-39.

Download:  PDF(1178KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The variations of structures and properties of some structural steelssubjected to tempering at a series of temperature after austempering or continuouscooling at certain rates, have been investigated. Based on the experimental results,the behavior and mechanism of the tempered bainite embrittlement have been dis-cussed.
Key words:  austempering      tempered bainite embrittlement      mechanical stability     
Received:  18 February 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I2/34

1 Horn R M, Rifchie P O. Metall Trans. 1978; 9A 1039
2 Chen D M, Hu G L, Kang MK. Microstructure and Mechanical Behaviour of Materials, Proceedings of an International Symposium held in Xi'an Jiaotong Univ., Xi'an, China, EMAS, 1985: 911
3 胡光立,华文君,康沫狂.航空材料,(专刊),1985;5(1) :1
4 Baker A J, Lauta F J, Wei R P. ASTM STP 370,1965: 3
5 刘正堂,康沫狂,杨峥.航空学报,1985;6:230
6 康沫狂.材料科学进展,1988;2(3) :12
7 徐祖耀.马氏体相变与马氏体,科学出版社,1980:462
8 黄麟綦,杨峥,胡光立,康沫狂,刘炳熙,聂玲娣.第三届国际材料热处理大会论文选集,机械工业出版社,1985:138
[1] Junjun CUI,Liqing CHEN,Haizhi LI,Weiping TONG. TEMPERED MICROSTRUCTURE AND MECHANICAL PROPERTIES OF AUSTEMPERED LOW ALLOYED BAINITIC DUCTILE IRON[J]. 金属学报, 2016, 52(7): 778-786.
[2] Shenghua ZHANG,Pei WANG,Dianzhong LI,Yiyi LI. INVESTIGATION OF TRIP EFFECT IN ZG06Cr13Ni4Mo MARTENSITIC STAINLESS STEEL BY IN SITU SYNCHROTRON HIGH ENERGY X-RAY DIFFRACTION[J]. 金属学报, 2015, 51(11): 1306-1314.
[3] ZHANG Peng ZHANG Fucheng WANG Tiansheng. PREPARATION AND MICROSTRUCTURE OF HARD BAINITE IN SURFACE LAYER OF CARBURIZED 20CrMnMoAl STEEL[J]. 金属学报, 2011, 47(8): 1038-1045.
No Suggested Reading articles found!