Please wait a minute...
Acta Metall Sin  1989, Vol. 25 Issue (2): 155-156    DOI:
Current Issue | Archive | Adv Search |
LIQUIDUS OF Ag-Cu-Ge PHASE DIAGRAM
LIU Shuqi;YI Tao Department of Chemistry; Peking University
Cite this article: 

LIU Shuqi;YI Tao Department of Chemistry; Peking University. LIQUIDUS OF Ag-Cu-Ge PHASE DIAGRAM. Acta Metall Sin, 1989, 25(2): 155-156.

Download:  PDF(140KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Thirteen internal sections of Ag-Cu-Ge phase diagram have been determined bymeans of DTA technique. Liquidus of the phase diagram has been constructed with the data ofinternal sections.
Key words:  Ag-Cu-Ge system      liquidus     
Received:  18 February 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I2/155

1 刘淑祺,孙文庆,金属学报,1988;24:B382
2 Hansen M. Constitution of Binary Alloys, 2nd ed., New York: McGraw-Hill, 1958: 18, 23, 585
3 Nowotny H, Bachmayer K. Monatsh Chem, 1950; 8: 669
4 Dutkiewicz J, Massalski T B. Metall Trans, 1981; 12A: 773
[1] GAO Zhongtang, HU Rui, WANG Jun, YANG Jieren, LI Jinshan. EFFECT OF ELECTROMAGNETIC MELT TREATMENT NEAR LIQUIDUS ON THE FORMATION OF NON-DENDRITE MICROSTRUCTURE OF SUPERALLOY[J]. 金属学报, 2014, 50(12): 1471-1477.
[2] LIU Shuqi;YI Tao Department of Chemistry; Peking University; Beijing. LIQUIDUS OF Au-Cu-Si SYSTEM[J]. 金属学报, 1990, 26(4): 153-154.
[3] ZHENG Chaogui;JIN Jun;YE Yupu Peking University. LIQUIDUS OF NdCl_3-MgCl_2-LiCl SYSTEM[J]. 金属学报, 1989, 25(1): 147-149.
[4] QIU Yiming;ZHU Yaoxiao Institute of Metal Research; Academia Sinica; Shenyang. RULE OF SEGREGATION OF ALLOYING ELEMENTS IN CAST Ni-BASE SUPERALLOYS[J]. 金属学报, 1989, 25(1): 78-80.
[5] LIU Shuqi;SUN Wenqing Department of Chemistry; Peking University. LIQUIDUS OF Ag-Cu-Bi SYSTEM[J]. 金属学报, 1988, 24(5): 448-450.
No Suggested Reading articles found!