Please wait a minute...
Acta Metall Sin  1989, Vol. 25 Issue (2): 109-115    DOI:
Current Issue | Archive | Adv Search |
INTERMETALLIC COMPOUNDS AND THEIR FORMATION REACTIONS IN HIGH-TEMPERATURE REGION OF Fe-Cr-Mo SYSTEM
LIU Shicheng;HAMAGUCHI Yoshikazu;KUWANO Hisashi Dalian Railway Institute Muroran Institute of Technology; Japan
Cite this article: 

LIU Shicheng;HAMAGUCHI Yoshikazu;KUWANO Hisashi Dalian Railway Institute Muroran Institute of Technology; Japan. INTERMETALLIC COMPOUNDS AND THEIR FORMATION REACTIONS IN HIGH-TEMPERATURE REGION OF Fe-Cr-Mo SYSTEM. Acta Metall Sin, 1989, 25(2): 109-115.

Download:  PDF(627KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The stable ranges concerning composition and temperature have expe-rimentally been determined for the intermetallic compounds in high-temperature re-gion of Fe-Cr-Mo system. The isothermal section of the Fe-Cr-Mo ternary phasediagram at 1250℃ and the formation reaction for the imtermetallic compounds,which are different in part from those shown in the literature have been proposed.
Key words:  Fe-Cr-Mo system      R-phase      χ-phase      σ-phase      μ-phase     
Received:  18 February 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I2/109

1 Wada T. Metals Handbook, 8th ed., Vol. 8: Metallography Structures and Phase Diagiams, ASM, 1973: 421
2 Raynor G V. Rivlin V G. Int Metall Rev, 1984; 29 (5) : 329
3 Sinha A K. Buckley R A. Hume-Rothery W. J Iron Steel Inst, London, 1967; 205: 191
4 武田修三,汤川夏夫.日本金属学会志,1957;21:275
5 Bechtoldt C J, Vacher H C. J Res Nat Bur Stand, 1957; 58: 7
6 Goldschmidt H J. Iron and Steel Inst, Special Report, №43, 1951: 249
7 Goldschmidt H J. Trans ASM, 1954; 46: 807
8 Goldschmidt H J. Metallurgia, 1957; 56: 17
9 高武盛,西沢泰二.日本金属学会志,1979;43:118
10 Komura Y, Sly W G. Shoemaker D P. Acta Crystallogr, 1960; 13: 575
11 刘世程.日本东北大学博土论文,1987
12 Dyson D J, Keown S R. Acta Metall, 1969; 17: 1096
13 Hughes H, Keown S R. J Iron Steel Inst, London, 1968; 206: 275
14 VerSnyder F L, Beattie H J Jr. Trans ASM, 1955; 47: 212
15 McMullin J G, Reiter S F, Ebeling D G. Trans ASM, 1954; 46: 799
[1] WU Tiyan;WU Qibai;Y. Riquier Central-South University of Technology; Changsha; Faculte Polytechnique de Mons; Belgium. MECHANICAL PROPERTIES AND б-PHASE EMBRITTLEMENT IN A FERRITE-AUSTENITE STAINLESS STEEL AT ELEVATED TEMPERATURES[J]. 金属学报, 1993, 29(2): 31-36.
[2] GUO Shouren;LU Dezhong;GUO Jianting;WU Xi Institute of Metal Research; Academia Sinica; Shenyang Fushun Steel Works associate professor. EFFECTS OF AGING TEMPERATURE AND TIME ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF GH35A SUPERALLOY[J]. 金属学报, 1990, 26(4): 32-39.
[3] ZHUANG Yinghong Guangxi University; Nanning. BEHAVIOUR OF Co_5 Cr_3 Si_2 PHASE IN Cu-RICH ALLOYS CONTAINING Co, Cr AND Si[J]. 金属学报, 1988, 24(6): 521-523.
No Suggested Reading articles found!