Please wait a minute...
Acta Metall Sin  1989, Vol. 25 Issue (1): 147-149    DOI:
Current Issue | Archive | Adv Search |
LIQUIDUS OF NdCl_3-MgCl_2-LiCl SYSTEM
ZHENG Chaogui;JIN Jun;YE Yupu Peking University
Cite this article: 

ZHENG Chaogui;JIN Jun;YE Yupu Peking University. LIQUIDUS OF NdCl_3-MgCl_2-LiCl SYSTEM. Acta Metall Sin, 1989, 25(1): 147-149.

Download:  PDF(199KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The liquidus of ternary system NdCl_3-MgCl_2-LiCl has been determined by meansof DTA. It was found that there are two surfaces corresponding to the primary crystallization ofNdCl_3 and α-(MgCl_2, LiCl) respectively, and an univariant line related to the secondary crystal-lization with a minimun point M (68.5 wt-% NdCl_3, 2.7 wt-% MgCl_2, 28.8 wt-% LiCl, 441℃)in the system.
Key words:  NdCl_3      NdCl_3-MgCl_2-LiCl      ternary system      liquidus     
Received:  18 January 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I1/147

1 张翊凤,郑朝贵,叶于浦.第四届全国熔盐化学及电化学学术会议论文集,郑州,1987:130
2 #12
3 Vogel G, Schneider A. Inorg Nucl Chem Lett, 1972; 8: 513
4 Sandonnini C. Atti Accad Naz Lincei Rend. Classe Sci Fis, Mat Nat, 1931; 22 (5) : 631
5 郑朝贵,张亚钢,陈集林,叶于浦.北京大学学报(自然科学版),1987;(6) :72
6 郑朝贵,叶于浦.高等学校化学学报,1988;9(5) :423
7 郑朝贵,靳军,叶于浦.中国稀土学报,(待发表
[1] GAO Zhongtang, HU Rui, WANG Jun, YANG Jieren, LI Jinshan. EFFECT OF ELECTROMAGNETIC MELT TREATMENT NEAR LIQUIDUS ON THE FORMATION OF NON-DENDRITE MICROSTRUCTURE OF SUPERALLOY[J]. 金属学报, 2014, 50(12): 1471-1477.
[2] Lü Baochen LIU Haitao REN Xin WANG Xiaoliang LI Gang SUN Yuejun. AN ATOM DENSE PACKING MODEL FOR METALLIC GLASS WITH HIGH SOLUTE CONCENTRATION IN (PSEUDO–) TERNARY SYSTEMS[J]. 金属学报, 2012, 48(2): 240-244.
[3] . Quasicrystals in Al-Cu-Ni-Fe Quaternary System[J]. 金属学报, 2007, 43(4): 374-378 .
[4] LI Juntao; HAO Shiming; WAN Qingfeng (Department of Materials Science and Engineering; Northeastern University; Shenyang 110006)Correspondent: HAO Shiming; professor; Tel: (024)23893000-7737; E-mail: smhao@mail. neu. eds. cn. STUDY ON α/γ PHASE EQUILIBRIUM IN Ti-Al-Cr-Fe QUARTERNARY SYSTEM[J]. 金属学报, 1998, 34(9): 897-902.
[5] XU Kuangdi;JIANG Guochang; ZHANG Xiaobing; TANG Kai; XU Jianlun; DING Weizhong (Shanghai Enhaned Laboratory of Ferrometallurgy; Shanghai University; Shanghai 200072). THE NEW DEVELOPMENT OF THE SELF-SReM4 MODEL AND ITS APPLICATION TO THE QUARTERNARY SYSTEM OF C-Mn-Fe-Si[J]. 金属学报, 1998, 34(5): 459-466.
[6] DING Jinjun;ZHAO Gang;HAO Shiming (Department of Materials Science and Engineering; School of Materials and Metallurgy; Northeastern University;Shenyang 110006). PHASE EQUILIBRIUM RELATIONSHIPS OF α_2(α)/γ IN THE Ti-Al-Cr TERNARY SYSTEM[J]. 金属学报, 1998, 34(2): 171-175.
[7] YU Jin (Shenyang Polytechnic University; Shenyang 110023) YU Yongli; WANG Zhichang (Northeastern University; Shenyang 110006)(Manuscript received 1996-04-03). MUTUAL SEPARATION OF RARE EARTH CHLORIDE MIXTURES USING A DRY PROCESS[J]. 金属学报, 1997, 33(4): 391-394.
[8] SHEN Jianyun; HAO Yaowu; ZHOU Chuanhua; LING Ling (General Research Institule for Non-Ferrous Metals; Beijing 100088). A MODEL WITH QUANTIFIED ASYMMETRY FOR PREDICTING THERMODYNAMIC PROPERTIES OF TERNARY SYSTEM[J]. 金属学报, 1996, 32(9): 943-948.
[9] LI Juntao; HAO Shiming (Northeastern University; Shenyang 110006). ^^α(α_2)/ PHASE EQUILIBRIA IN Ti-Al-Si SYSTEM[J]. 金属学报, 1996, 32(11): 1171-1176.
[10] CHE Guangcan Institute of Physics; Academia Sinica; Beijing; ELLNER M. Max-Planck-Institut for Metallforschung; Stuttgart; Germany. PHASE DIAGRAM OF Bi-Pb-Tl TERNARY SYSTEM[J]. 金属学报, 1991, 27(6): 152-154.
[11] ZHANG Kanghou;CHEN Lili Institute of Precious Metals; Kunming. ROOM TEMPERATURE AND 700℃ ISOTHERMAL SECTIONS OF Gd-Pd-Pt(Gd≤33 at. -%) PHASE DIAGRAM[J]. 金属学报, 1991, 27(3): 147-149.
[12] LIU Shuqi;YI Tao Department of Chemistry; Peking University; Beijing. LIQUIDUS OF Au-Cu-Si SYSTEM[J]. 金属学报, 1990, 26(4): 153-154.
[13] CHEN Rongzhen;ZHANG Hanxing;ZHENG Jianxuan;HE Hanping Guangxi University; Nanning Guangxi Institute of Non-Ferrous Metals Geology; Nanning CHEN Rongzhen;Department of Physics;Guangxi University; Nanning;530009 Guangxi. 410℃ ISOTHERMAL SECTION OF Al-Cu-Sb TERNARY SYSTEM PHASE DIAGRAM[J]. 金属学报, 1989, 25(5): 142-143.
[14] ZHANG Kanghou;CHEN Lili Kunming Institute of Precious Metals ZHANG Kanghou; Kunming Institute of Precious Metals; 650221 Kunming. ROOM TEMPERATURE AND 750℃ ISOTHERMAL SECTIONS OF Ag-Pd-Gd TERNARY SYSTEM (Gd≤25 at.-%) PHASE DIAGRAM[J]. 金属学报, 1989, 25(5): 139-141.
[15] LIU Shuqi;YI Tao Department of Chemistry; Peking University. LIQUIDUS OF Ag-Cu-Ge PHASE DIAGRAM[J]. 金属学报, 1989, 25(2): 155-156.
No Suggested Reading articles found!