| APPLICATION OF MAXIMUM ENTROPY METHOD TO CALCULATE RDF OF Ni-P AMORPHOUS ALLOY FROM X-RAY DIFFRACTION DATA |
| LIANG Jianduan;LIN Shuzhi Institute of Metal Research; Academia Sinica; Shenyang |
|
Cite this article:
LIANG Jianduan;LIN Shuzhi Institute of Metal Research; Academia Sinica; Shenyang. APPLICATION OF MAXIMUM ENTROPY METHOD TO CALCULATE RDF OF Ni-P AMORPHOUS ALLOY FROM X-RAY DIFFRACTION DATA. Acta Metall Sin, 1989, 25(1): 141-146.
|
|
|
Abstract Experiments clarified that the application of maximum entropymethod to calculate the RDF (radial distribution function) of the Ni-P amorphousalloy from its X-ray diffraction data shows a higher resolution and good consistentwith know results with less data. It is believed that this method is available forthe analysis of amorphous structure.
|
|
Received: 18 January 1989
|
1 魏文铎,物理学报,1986:35:171 2 Wei Wendo (魏文铎). J Non-Cryst Solids, 1986; 81: 239 3 林树智,黑祖昆,物理学报,1984;33:302 4 Wei Wendo (魏文铎). J Appl Crystallogr, 1985; 18: 442 5 Wei Wendo (魏文铎). Chinese J Met Sci Technol, 1987; 3: 214 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|