Please wait a minute...
Acta Metall Sin  1988, Vol. 24 Issue (6): 518-520    DOI:
Current Issue | Archive | Adv Search |
LOCAL EQUILIBRIUM METHOD IN STUDYING PHASE DIAGRAM OF Mn-MnO SYSTEM
CHEN Qiyuan Central South University of Technology; Changsha
Cite this article: 

CHEN Qiyuan Central South University of Technology; Changsha. LOCAL EQUILIBRIUM METHOD IN STUDYING PHASE DIAGRAM OF Mn-MnO SYSTEM. Acta Metall Sin, 1988, 24(6): 518-520.

Download:  PDF(205KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A special method based on the local equilibrium principle has been introduced inthe research of the phase diagram of Mn-MnO system. With this method, the difficulties of vol-atilization of Mn and the corrosion of Mn and MnO to refractory material were avoided. Thesolubility of oxygen in Mn and the composition of the interface between MnO and Mn weredetermined. Parts of the phase diagram of Mn-MnO system were constructed according to exper-imental results.
Key words:  Local equilibrium method      Mn-MnO system      phase diagram     
Received:  18 June 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I6/518

1 陈启元,锰-氧系相图与二氧化锰热分解动力学,中南工业大学博士论文,1986
2 Schenck H, Frohberg M G, Nunninghoff R. Arch Eisenhuttenwes, 1964; 35: 269
3 Picard C, Gerdanian P. J Solid State Chem, 1974; 11: 190
4 Klingsberg C, Roy R. J Am Ceram S?c, 1960; 43: 620
5 Eror N G. Wagner J B Jr., J Electr?chem s?c, 1971; 118: 1665
6 B?cquet J-P, Kawahara M, Lacombe P. C R Hebd Seances Acad Sci (Paris), 1967; C265: 1318
[1] GAO Xiang, ZHANG Guikai, XIANG Xin, LUO Lizhu, WANG Xiaolin. Effects of Alloying Elements on the Adsorption of Oxygen on V(110) Surfaces: A First-Principles Study[J]. 金属学报, 2020, 56(6): 919-928.
[2] ZHANG Weibin SHA Chunsheng DU Yong WEN Guanghua XIE Wen WANG Shequan. COMPUTER SIMULATIONS AND VERIFICATION OF GRADIENT ZONE FORMATION IN CEMENTED CARBIDES[J]. 金属学报, 2011, 47(10): 1307-1314.
[3] ZHANG Huawei; LI Yanxiang; LIU Yuan. Study of Metal--Hydrogen Binary Phase Diagram in Gasar Process[J]. 金属学报, 2005, 41(1): 55-.
[4] ZHANG Jian(Metallurgical Engineering School; University of Science and Technology Beijing; Beijing 100083). CONSISTENCY(OR SIMILARITY) OF THERMODYNAMIC PROPERTIES OF METALLURGICAL MELTS WITH THEIR PHASE DIAGRAMS[J]. 金属学报, 1998, 34(7): 742-752.
[5] Zhang Jian (Institute of Metallurgy; University of Science and Technology Beijing; Beijing 100083). CLASSIFICATION OF THERMODYNAMIC PROPERTIES OF BINARY METALLIC MELTS ACCORDING TO THEIR PHASE DIAGRAMS[J]. 金属学报, 1998, 34(1): 75-85.
[6] ZHOU Hong; WANG Jinguo; JIA Shusheng (Jilin University of Technology; Chanerhun 130025) OGIKeisaku(Kyushu Universily; Japan) (Manuscript received 1996-03-22; in revised form 1997-04- 13). SOLIDIFIED MICROSTRUCTURES AND PHASES OF HIGH SPEED STEELS CONTA1NING DIFFERENT V AND C CONTENT[J]. 金属学报, 1997, 33(8): 838-843.
[7] FANG Jianhui; TANG Yun; LI Yu; YAN Licheng; CHEN Nianyi (Shanghai University;Shanghai 201800); WANG Jiyang (Shandong University; Jinan 250012)(Manuscript received 1996-04-08; in revised form 1996-09-10). KPO_3-M0O_3 PHASE DIAGRAM[J]. 金属学报, 1997, 33(4): 395-397.
[8] ZHOU Guozhi(Kuo-Chih Chou) (University of Science and Technology Beijing;Beiing 100083). NEW GENERATION SOLUTION GEOMETRICAL MODEL AND ITS FURTHER DEVELOPMENT[J]. 金属学报, 1997, 33(2): 126-132.
[9] DING Jinjun;ZHAO Gang;HAO Shiming (Northeastern University; Shenyang 110006). PHASE EQUILIBRIUM RELATIONSHIPS AND INTERDIFFUSION COEFFICIENTS OF β,α ANDγIN THE Ti-Al BINARY SYSTEM[J]. 金属学报, 1997, 33(10): 1105-1109.
[10] YUAN Wenxia; MA Shulan; QIAO Hin; ZHUANG Weidong; XING Xianran;QIAO Zhiyu (University of Science and Technology Beijing; Beijing 100083)(General Institute for Non-Ferrous Metals; Beijing 100088)(Manuscript received 1995-04-28; in revised form 1995-11-05). A STUDY ON THE YCl_3-AECl_2(AE=Mg, Ca, Sr, Ba)BINARY PHASE DIAGRAMS[J]. 金属学报, 1996, 32(2): 139-143.
[11] HAO Shiming; ZENG Ninghua (Northeastern University; Shenyang 110006)(Manuscript received 1994-11-16). ISOTHERMAL SECTION OF PHASE DIAGRAM IN Ti-Al-Cr TERNARY SYSTEM AT 1000℃[J]. 金属学报, 1995, 31(16): 152-158.
[12] YAN Licheng;FANG Jianhui;XU Jingyan;YANG Jinxiu(Shanghai University of Science and Technology). PHASE DIAGRAM OF KF-LiCl-CaCl_2 SYSTEM[J]. 金属学报, 1994, 30(19): 301-303.
[13] WAN Jinglong(Anhui Institute of Technology; Hefei); BI Qinghua(Shanghai University of Science and Technology). Gd-CoAl VERTICAL SECTION OF Gd-Co-Al PHASE DIAGRAM[J]. 金属学报, 1994, 30(17): 204-207.
[14] XU Qian;YU Yaxin;QIU Zhuxian(Northeastern University;Shenyang)(Manuscript received 25 June;1993). THERMODYNAMIC PROPERTIES AND PHASE DIAGRAMS OF Li-CaF_2,NaF-CaF_2 AND KF-CaF_2[J]. 金属学报, 1994, 30(16): 150-155.
[15] SHEN Jianyun(General Research Institute for Non-Ferrous Metals;Beijing);CHATILLON C(Laboratoire de Thermodynamique et Physico-chimie Metallurgiques;Fracne)(Manuscript received 16 June;1993). THERMODYNAMICS OF Ga-In-As SYSTEM UNDER LATTICE DEFORMATION[J]. 金属学报, 1994, 30(16): 145-149.
No Suggested Reading articles found!