ELECTROCHEMICAL STUDIES ON ANODIC DISSOLUTION OF SYNTHETIC NICKEL SULPHIDES
FANG Zhaoheng;CHEN Jiayong Institute of Chemical Metallurgy; Academia Sinica; Beijing
Cite this article: 

FANG Zhaoheng;CHEN Jiayong Institute of Chemical Metallurgy; Academia Sinica; Beijing. ELECTROCHEMICAL STUDIES ON ANODIC DISSOLUTION OF SYNTHETIC NICKEL SULPHIDES. Acta Metall Sin, 1988, 24(6): 463-470.

Download:  PDF(643KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The anodic behaviours of synthetic nickel sulphides in H_2SO_4 solutionwere studied. When the anodes of Ni_3S_2, Ni_7S_6 and NiS are actively dissolved respec-tively, a solid layer is formed on the electrode surface with its nature and com-position depend on the applied potential. Based on the electrochemical Phenomena,phase and elemental compositions of the solid layer formed on the electrode surfacewere determined. The apparent number of electrons transfered during dissolution ofone Ni~(2+) was also measured. It can be considered that there are three parallel reac-tions occurred on the electrode: the reaction with formation of HSO_4~- or SO_4~(2-), thereaction with formation of sulphides as intermediates and the reaction of formingelemental S. With NiS_2, as an anode, formation of SO_4~(2-). or HSO_4~- can be consider-ed as the only reaction ocurred on the electrode.
Key words:  nickel sulphide      anodic dissolution      electrochemical behaviour     
Received:  18 June 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I6/463

1 Kullevuel G, Yund R A. J Petrol, 1962; 3: 126
2 Rau H. J Phys Chem Solids, 1975; 36: 1199 Rau H. J Phys Chem Solids, 1976; 37: 929
3 Kato T, Ori T. J Jpn Inst Met, 1973; 37: 1338
4 #12
5 秦毅红,赵瑞荣,蒋汉瀛.中南矿冶学院内部资料,1983
6 Price D C, Davenport W G. J Appl Electrochem, 1982; 12: 281
7 Yamauch C, Kamentani H, Kammel P. Metall, 1981; 35: 401
8 花田直纪,岸富也,永井隆.电气化学与工业物理化学,1981;49:712
9 Power G P. Aust J Chem, 1981; 34: 2297
10 蒋汉瀛,舒余德,张征林.中南矿冶学院学报,1983;(4) :100
11 Scharrifker B, Hills G. Electrochem Acta, 1983; 27: 879
12 Sato S, Cohen M. J Electrochem Soc, 1964; 111: 517
13 Vanghan D J, Craig J R. Mineral Chemistry of Metal Sulfides, Cambridge University Press, 1978: 322k
[1] SONG Renguo; ZHANG Baojin; ZENG Meiguang(Northeastern University; Shenyang 110006)(State Key Laboratory of Solidification Processing; Northwestern PolytechnicalUniversity; Xi'an 710072). THE STRESS CORROSION AND ROLE OF Mg SEGREGATED TO GRAIN BOUNDARY IN 7175 ALUMINIUM ALLOY[J]. 金属学报, 1997, 33(6): 595-601.
[2] HUANG Yizhong; CHEN Qizhi; CHU Wuyang (University of Science and Technology Beijing; Beijing 100083)(Manuscript received 1995-03-28; in revised form 1995-07-03). IN SITU TEM OBSERVATION OF SCC IN 310 STAINLESS STEEL[J]. 金属学报, 1996, 32(1): 39-45.
[3] HUANG Yizhong(Beijing Instilute of Aeronautic Materials);CHEN Qizhi(University of Science and Technology Beijing);YUAN Changyan(Beijing Institute of Aeronautic Malerials);CHU Wuyang(University of Science and Technology. Beijing). IN SITU TEM OBSERVATIONS OF DISLOCATION EMISSION, MULTIPICATION AND MOTION INDUCED BY ANODIC DISSOLUTION IN TYPE 310 STAINLESS STEEL[J]. 金属学报, 1994, 30(22): 453-458.
[4] WEI Xuejun;LI Jin;ZHOU Xiangyang;KE Wei(Corrosion Scicnce Laboratory; Institute of Corrosion and Protection of Metals; Chinese Academy of Scicnces;Shenyang). SURFACE AND BULK DEFORMATION NEAR CRACK TIP FOR PURE COPPER UNDER APPLIED ANODIC CURRENT[J]. 金属学报, 1994, 30(21): 393-397.
[5] CAO Chunan;LIN Haichao;LU Ming Corrosion Science Laborotory; Institute of Corrosion and Protection of Metals; Academia Sinica; ShenyangHUANG Yanliang;Ph D student;Institute of Corrosion and Protection of Metals ;Aeudemia Sinica;Shenyang 110015. SCC MECHANISM OF AISI 321 IN ACIDIC CHLORIDE SOLUTION[J]. 金属学报, 1993, 29(5): 68-73.
[6] WANG Zhengfu;ZHU Ziyong;KE Wei;ZHANG Yun;HU Zhuangqi Corrosion Science Laboratory; Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang; Institue of Metal Research; Academia Sinica; Shenyang. STRESS CORROSION PERFORMANCE OF Al-Li-Cu-Mg ALLOY[J]. 金属学报, 1992, 28(4): 58-62.
[7] LIU Ping;XU Changgan Beijing University of Aeronautics and Astronautics. ELECTROCHEMICAL BEHAVIOUR OF PHASES IN TITANIUM ALLOYS[J]. 金属学报, 1989, 25(4): 115-119.
No Suggested Reading articles found!