MAGNETIC PROPERTIES OF Nd_2(Fe_(1-x)M_x)_(14)B(M=C, Si) ALLOYS
XING Feng;JIANG Chao;HO Wenwang Department of Physics; Peking University
Cite this article: 

XING Feng;JIANG Chao;HO Wenwang Department of Physics; Peking University. MAGNETIC PROPERTIES OF Nd_2(Fe_(1-x)M_x)_(14)B(M=C, Si) ALLOYS. Acta Metall Sin, 1988, 24(5): 420-424.

Download:  PDF(426KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The magnetic properties of Nd_2(Fe_(1-x)M_x)_(14)B (M=C, Si) compoundshave been investigated. Substituting Fe by a small amount of metalloid C and Siatoms, the compounds are in tetragonal structure and have uniaxial anisotropy. Thesubstitution of C for part of Fe makes the Curie temperature and the intrinsic coer-civity of bond samples decrease at low temperature. The replacement of Fe by Simakes the Curie temperature increase with a maximum at the vicinity of x=0. 15.When the range of the content of Si is 0≤x≤0.10, the coercivity distinctly in-creases at room temperature, from 62.7 kA/m at x=0 to 138.7kA/m at x=0.06, wherethe residual magnetization has a maximum; at the mean time the saturation magne-tization decreases only by a small amount.
Key words:  Nd-Fe-B alloy      magnetic properties      Curie temperature     
Received:  18 May 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I5/420

1 Herbst J F, Croat J J, Yelon W B. J Appl Phys, 1985; 57: 4086
2 Matsuura Y. Hirosawa S, Yamamo to H, Fujimura S, Sagawa M. Appl Phys Lett, 1985; 46: 308
3 Yang Y C (杨应昌), Ho W W (何文望), Chen H Y (陈海英), Wang J (王进), Lan J (兰健). J Appl Phys, 1985; 57: 4118
4 Abache C, Oesterreicher H. J Appl Phys, 1986; 57: 1114
5 Liuingston J D. Proc 8th Int Wokshop on Rare-Earth Magnets and their Applioations 1985: 423
6 杨应昌,何文望,陈海英,邢峰,兰健,中国稀土学报,1985;3(2) :34
7 Sucksmith W, Thompson J E. Proc Roy Soc London, Ser. A, 1954; 225: 362
8 Koon N C, Das B N, Rubinstein M, Tyson J. J Appl Phys, 1985; 57: 4091
9 Givord D, Li H S, Perrier de la Bathie R. Solid State Commun, 1984; 51: 857
[1] Jiaojiao DU,Guojian LI,Qiang WANG,Yonghui MA,Huimin WANG,Mengmeng LI. GROWTH MODE EVOLUTION AND SUBSEQUENT MAGNETIC PROPERTIES OF Fe FILMS WITH DIFFERENT GRAIN SIZES UNDER A HIGH MAGNETIC FIELD[J]. 金属学报, 2015, 51(7): 799-806.
[2] WANG Dongmei SONG Lin WANG Yaohui ZHANG Wei Bilige Tegus O. MAGNETOCALORIC EFFECT IN MnFeP0.63Ge0.12Si0.25Bx (x=0, 0.01, 0.02, 0.03) COMPOUNDS[J]. 金属学报, 2011, 47(3): 344-348.
[3] LIANG Haining SONG Xiaoyan ZHANG Zhexu LU Nianduan LIU Xuemei ZHANG Jiuxing. PREPARATION AND CHARACTERIZATION OF SmCo2 NANOCRYSTALLINE ALLOY WITH PERMANENT MAGNETIC PROPERTIES[J]. 金属学报, 2010, 46(8): 973-978.
[4] Gao-Feng WANG; Lin SONG. Magnetocaloric effect on low field in non-stoichiometric MnFe(P,Si,Ge) alloys[J]. 金属学报, 2007, 43(8): 889-892 .
[5] XU Min; SUN Yu; QUAN Mingxiu; WANG Y; ong; ZUO Liang. Glass--Forming Ability and Soft Magnetic Properties of Fe--Co--Nd--Nb—B Amorphous Alloys[J]. 金属学报, 2007, 43(7): 699-704 .
[6] YIN Xiaoying;WANG Yingang;TANG Ning;YANG Fuming(State Key Laboratory of Magnetism; Institute of Physics; Chinese Academy of Sciences; Beijing 100080)(Chinese People's Public Security University; Beijing 100038). CRYSTAL STRUCTURE AND MAGNETIC PROPERTIES OF Y_2Fe_(17-x)Mn_x[J]. 金属学报, 1997, 33(5): 539-542.
[7] WANG Zhi;HE Kaiyuan;ZHANG Luo (Northeastern University; Shenyang 110006)(Tianjin Institute of Technology; Tianjin 300191)(Shanghai Iron and Steel Research Institute; Shanghai 200940). MAGNETOTHERMAL ANALYSIS OF Fe_(72.7)Cu_1Nb_2V_(1.8)Si_(13.5)B_9 ALLOY[J]. 金属学报, 1997, 33(12): 1289-1294.
[8] YANG Jilian;ZHANG Baisheng;DING Yongfan;YANG Yingchang;ZHANG Xiaodong;PAN Shuming China Institute of Atomic Energy; Beijing Department of Physics; Peking University; Beijing General Research Institute for Non-Ferrous Metals; Beijing associate professor; P.O. Box 275; Branch No.30; Beijing 102413. NEUTRON DIFFRACTION STUDY ON R_2Fe_(17)N_χ(R=Y, Dy, Nd)[J]. 金属学报, 1993, 29(3): 84-87.
[9] SHEN Baogen;KONG Linshu;CAO Lei;WANG Fangwei;ZHAN Wenshan;GUO Huiqun;ZHAO Jiangao State Key Laboratory of Magnetism; Institute of Physics; Academia Sinica. INFLUENCE OF INTERSTITIAL CARBON ATOMS ON FORMATION, STRUCTURE AND MAGNETIC PROPERTIES OF (Er_(1-x)Sm_x)_2Fe_(17)C_y COMPOUNDS[J]. 金属学报, 1993, 29(10): 76-81.
[10] HU Fengxia;CHEN Jinchang;SHEN Baogen;GUO Huiqun Institute of Physics; Academia Sinica; Beijing; Beijing Teacher's College; Institute of Physics; Academia Sinica; Beijing. MAGNETIC PROPERTIES AND CRYSTALLIZATION OF AMORPHOUS ALLOYS Co_(90-x)Cr_xZr_(10)[J]. 金属学报, 1992, 28(2): 71-76.
[11] CAO Lei; SHEN Baogen; YANG Linyuan; ZHAO Jiangao (State Key Laboratory of Magnetism; Institute of Physics; Academia Sinica; Beijing). MAGNETIC PROPERTIES AND CRYSTALLIZATION OF AMORPHOUS Nd_4Fe_(77.5)(B_(1-x)C_x)_(18.5) ALLOYS[J]. 金属学报, 1992, 28(11): 70-74.
[12] GU Benxi;ZHAI Hongru;SHEN Baogen Department of Physics; Nanjing University; Nanjing Institute of Physics; Academia Sinica; Beijing. CRYSTALLIZATION AND MAGNETICPROPERTIES OF AMORPHOUS Nd_6Fe_(81)B_(13) ALLOY[J]. 金属学报, 1990, 26(5): 102-106.
[13] SHEN Baogen;ZHANG Zhiying;GUO Huiqun;ZHAO Jiangao;GU Benxi Institute of Physics; Academia Sinica; Beijing Department of Physics; Nanjing University research assistant. MAGNETIC MOMENT, CURIE TEMPERATURE AND SPIN WAVE EXCITATION FOR AMORPHOUS Fe_(90-x) Si_x Zr_(10) ALLOYS[J]. 金属学报, 1990, 26(4): 119-124.
[14] GUAN Kehong;WANG Jun Northeast University of Technology; Shenyang GUAN Kekong; associate professor; Department of Material Science and Engineering;Northeast University of Technology; 110006 Shenyang. INTRINSIC MAGNETISM AND MAGNETIC ANISOTROPY OF AMORPHOUS ALLOYS Fe_(1-x)(Si, B)_x[J]. 金属学报, 1989, 25(5): 111-114.
[15] GUAN Kehong;PU Xiaodong Northeast University of Technology; ShenyangDept. Mater. Sci.; Northeast University of Technology;Shenyang. MAGNETIC MOMENT AND CURIE TEMPERATURE OF (Fe_(80)Ni_(20))_(78)Si_(22-x)B_x AMORPHOUS ALLOYS[J]. 金属学报, 1988, 24(3): 296-298.
No Suggested Reading articles found!