| THEORETICAL CALCULATION OF SPECIFIC INTERFACIAL ENERGY OF SEMICOHERENT INTERFACE BETWEEN MICROALLOY CARBONITRIDES AND AUSTENITE |
| YONG Qilong;LI Yongfu;SUN Zhenbao;WU Baorong Yunnan Institute; of Technology;Kunming; Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing |
|
Cite this article:
YONG Qilong;LI Yongfu;SUN Zhenbao;WU Baorong Yunnan Institute; of Technology;Kunming; Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing. THEORETICAL CALCULATION OF SPECIFIC INTERFACIAL ENERGY OF SEMICOHERENT INTERFACE BETWEEN MICROALLOY CARBONITRIDES AND AUSTENITE. Acta Metall Sin, 1988, 24(5): 373-375.
|
|
|
Abstract According to the misfitting dislocation theory, a method of theoretical calculationwas developed for the spedific energy of the semicoherent interface between microalloy carboni-trides and austenite matrix. The calculating formulae were derived and the results were satifac-torily applied on the research works.
|
|
Received: 18 May 1988
|
1 Hannerz N E, De Kazinczy F. J Iron Steel Inst, 1970; 208: 475 2 Weiss I, Jonas J J. Metall Trans. 1980; 11A: 403 3 Matthews J W In: Nabarro F R N ed., Dislocations in Solids Vol. Ⅱ, Amsterdam: North-Holland, 1979; 461 4 Van der Merwe J H, Woltersdorf J, Jesser W A. Mater Sci Eng, 1986; 81: 1 5 Davenport A T. Brossard L C, Miner R E. J Met, 1975; 27(6) : 21 6 Chang Y A, Toth L E, Tyan Y S. Metall Trans, 1971; 2: 315 7 Nabarro F R N. Theory of Crystal Dislocations, Oxford: C Clarendon, 1967: 130, 137 8 Brandes E A. In: Smichells C J ed., Smithells Metals Refference Book, 6th ed., London: Butter-worths, 1983: 9 Koster W. Z Metall, 1948; 39: 1 10 雍岐龙,微合金钢中微合金碳氮化物在奥氏体中的沉淀问题,冶金工业部钢铁研究总院博士论文,19877 |