DETERMINATION OF SPACE GROUP OF PrCo_(12)B_6 COMPOUND BY COVERGENT BEAM ELECTRON DIFFRACTION
WANG Fuhui;BIAN Weimin Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang; Northeast University of Technology; Shenyang
Cite this article: 

WANG Fuhui;BIAN Weimin Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang; Northeast University of Technology; Shenyang. DETERMINATION OF SPACE GROUP OF PrCo_(12)B_6 COMPOUND BY COVERGENT BEAM ELECTRON DIFFRACTION. Acta Metall Sin, 1988, 24(4): 368-370.

Download:  PDF(413KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The space group of PrCo_(12)B_6 compound has been determined using the convergentbeam electron diffraction method. The space group is found to be R3m.
Key words:  convergent beam electron diffraction      space group      PrCo_(12)B_6 compound     
Received:  18 April 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I4/368

1 Niinara K, Yajima S, Chem Lett, 1972; (10) : 875
2 #12
3 ElMasry N A, Stadelmaier H H. J Less-Common Met, 1984; 96: 165
4 Chuang Y C, Wu C H, Wang F H. J Less-Common Met, 1987; 135: 5
5 Hahn T. International Tables for Crystallography, Vol. A, Holland, Boston: Reidel, 1983: 534
6 Buxton B F, Eades J A, Steeds J W, Raokham G M. Philos Trans Roy Soc London, Ser. A1976; 281: 171
7 Tanaka M, Saito R, Sekii H, Acta Crystallogr, 1983; A39: 357
[1] BIAN Weimin ZHU Yimei ZHOU Lian. DETERMINATION OF SPACE GROUP OF INCOMMENSURATE MODULATION STRUCTURE PHASES IN Bi HIGH TEMPERATURE SUPERCONDUCTORS[J]. 金属学报, 2009, 45(6): 673-679.
No Suggested Reading articles found!