Please wait a minute...
Acta Metall Sin  1988, Vol. 24 Issue (4): 371-372    DOI:
Current Issue | Archive | Adv Search |
Bi-Sr-Ca-Cu OXIDE SUPERCONDUCTOR WITH ZERO RESISTANCE TEMPERATURE 85.3K
SHI Fan;ZHOU Shouzeng;SHI Zhenhua;LI Fubiao Beijing University of Iron and Steel TechnologyDepartment of Materials Science and Engineering;Beijing University of Iron and Steel Technology; Beijing
Cite this article: 

SHI Fan;ZHOU Shouzeng;SHI Zhenhua;LI Fubiao Beijing University of Iron and Steel TechnologyDepartment of Materials Science and Engineering;Beijing University of Iron and Steel Technology; Beijing. Bi-Sr-Ca-Cu OXIDE SUPERCONDUCTOR WITH ZERO RESISTANCE TEMPERATURE 85.3K. Acta Metall Sin, 1988, 24(4): 371-372.

Download:  PDF(108KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The Bi-Sr-Ca-Cu-O superconducting ceramics with T_c (onset)=112K, T_c (R=0)=85.3K were prepared by quenching process. The Meissner effect of the sample appears at about84.0K.
Key words:  superconductivity      Bi-Sr-Ca-Cu-O system     
Received:  18 April 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I4/371

1 Michel C, Hervieu M, Borel M M. Grandin A, Deslandes F, Provost J, Raveau B. Z Phys B, 1987; 68: 421
2 Maeda H, Tanaka Y, Fukutomi M, Asano T. Jpn. J Appl Phys Part 2 Lett, 1988
[1] ZHANG Liuwan; CHEN Tingguo; XIE Xiaoming; WU Xiaochu; SHITiansheng(Shanghai Institute of Metallurgy; Chinese Academy of Sciences;Shanghai 200050) LI Xiangting; GAO Jianhua; SUN Jing(Shanghai Institute of Ceramics;Chinese Academy of Sciences; Shanghai 200050). EFFECTS OF HEAT TREATMENT ON Pb-DOPED Bi-2223 SUPERCONDUCTOR[J]. 金属学报, 1995, 31(6): 277-285.
[2] WANG Genmiao;ZHANG Han;ZHANG Qirui;WU Yonghua Centre of Structure and Elements Analysis; University of Science and Technology of China; Hefei. MOSSBAUER EFFECT STUDY OF YBa_2 Cu_(3-x)Sn_x o_(7-y) SYSTEM[J]. 金属学报, 1990, 26(5): 142-146.
[3] WEN Lishi;QIAN Shengwei;HU Qingyu;GUAN Kan;ZHUANG Yuzhi Institute of Metal Research; Academia SinicaInstitute of Metal Research;Academia Sinica;Shenyang. CHARACTERIZATION OF MICROSTRUCTURE OF PLASMA SPRAYED SUPERCONDUCTING COATING[J]. 金属学报, 1988, 24(3): 286-289.
No Suggested Reading articles found!