GROWTH OF ISOTHERMAL MARTENSITE IN AN Fe-Ni-Mn ALLOY
YANG Dazhi;ZHU Min Dalian Institute of Technology; LiaoningDept.of Mater.Sci. and Eng.;Dalian Institute of Technology; Liaoning
Cite this article: 

YANG Dazhi;ZHU Min Dalian Institute of Technology; LiaoningDept.of Mater.Sci. and Eng.;Dalian Institute of Technology; Liaoning. GROWTH OF ISOTHERMAL MARTENSITE IN AN Fe-Ni-Mn ALLOY. Acta Metall Sin, 1988, 24(4): 236-241.

Download:  PDF(2109KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The substructural development of martensite plates at different stageof the transformation for an Fe-21Ni-4Mn alloy has been investigated by usingtransmission electron microscope. Twinning was found in small thin platelets atthe initial stage. Fine twins extend to the whole platelet. The dislocations and twinswere found in the thick platelets at a later stage. Bending of the twins was alsoobserved frequently at this stage. Finally, several platelets coalesce with each otherto forma macroscopic (252)_f martensite "plate". The original habit plane of theindividual platelet was measured to be close to (121)_f.
Key words:  Fe-Ni-Mn alloy      plate martensite      isothermal transformation     
Received:  18 April 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I4/236

1 Pitsch W. Philos Mag, 1954; 4: 577
2 Nishiyama Z, Shimizu K, Sugino K. Acta Metall, 1961; 9: 620
3 Thomas C. Metall Trans, 1971; 2: 2373
4 Maki T, Wayman C M. Acta Metall, 1977; 25: 681
5 Oshima R, Wayman C M. Trans Jpn Inst Met, 1975; 16: 7
6 Tanaka Y, Shimizu K. Trans Jpn Inst Met, 1981; 22: 35
7 Yang D-Z, Wayman C M. Acta Metall, 1984; 32: 949
8 Yang D-Z, Wayman C M. Metallography, 1984; 17: 12
9 Yang D-Z, Sandvik B P J, Wayman C M. Metall Trans, 1984; 15A: 1555
10 Sandvik B P J, Wayman C M. Metall Trans, 1983; 14A: 2469
11 Sandvik B P J, Wayman C. M. Metall Trans, 1983; 14A: 2455
12 Kajiwara S. Philos Mag, 1981; A43: 1483U
[1] LU Wei;ZHENG Denghui;XU Zuyao Shanghai Jiao Tong UniversityDepartment of Materials Science;Shanghai JiaoTong University; Shanghai 200030.. INFLUENCE OF RARE EARTH ON TTT DIAGRAM FOR 0.27C-1Cr STEEL[J]. 金属学报, 1993, 29(7): 23-27.
[2] GONG Hai;ZHANG Weiyi Dalian Railway Institute; ZHANG Xiumu Institute of Metal Research; Academia Sinica; Shenyang. NUCLEATION AND GROWTH OF FERROUS MARTENSITES ALONG BOUNDARIES[J]. 金属学报, 1991, 27(3): 41-45.
[3] SUN Enxi;YANG Dazhi;XU Zuyao;YANG Fumiug;ZHAO Ruwen Dalian Institute of Railway Dalian University of Technology Shanghai Jiaotong University Institute of Physics; Academia Sinica; Beijing professor. PULSED MAGNETIC FIELD-INDUCED MARTENSITIC TRANSFORMATION IN AN Fe-21Ni-4Mn ALLOY[J]. 金属学报, 1990, 26(4): 12-17.
[4] YANG Liu;FANG Hongsheng;CHEN Nanping Tsinghua University; Beijing. DRIVING FORCE OF BAINITIC TRANSFORMATION FOR Fe-Mn-C ALLOYS[J]. 金属学报, 1989, 25(4): 30-35.
No Suggested Reading articles found!