INTERACTION BETWEEN Pb AND C, Pb AND Ce IN Fe-C-Pb, Fe-C_(sat)-Pb-Ce LIQUID SOLUTIONS
WANG Zhengyue;DU Ting;WANG Longmei Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing
Cite this article: 

WANG Zhengyue;DU Ting;WANG Longmei Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing. INTERACTION BETWEEN Pb AND C, Pb AND Ce IN Fe-C-Pb, Fe-C_(sat)-Pb-Ce LIQUID SOLUTIONS. Acta Metall Sin, 1988, 24(3): 236-241.

Download:  PDF(405KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The thermodynamic properties of Fe-C-Pb liquid solution in the tem-perature range 1300--1400℃ have been studied using the equilibrium method betweenPb vapour and liquid Fe in sealed Mo reaction chamber. The temperature depend-ence of the first and second order interaction coefficients between C and Pb areobtained as follows: e_(Pb)~C=9205(1/T)-4.578, γ_(Pb)~C=-1047(1/T)+0.512. The thermody-namic preperties of Fe-C_(sat)-Pb-Ce liquid solution at 1300℃ have been determinedusing the equilibrium method between vapour and liquid in a graphite cruciblesealed in a vacuum quartz tube. The interaction coefficients between Ce and Pb arederived to be: e_(Pb)~(Ce)=-2. 11, e_(Ce)~(Pb)=-1.43.
Key words:  Fe-C-Pb solution      Fe-C-Pb-Ce solution      Pb-C interaction      Pb-Ce interaction     
Received:  18 March 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I3/236

1 Du Ting, Wang Longmei. J Less-Common Met. 1985; 110: 179
2 王龙妹,杜挺.钢铁,1985;20(8) :9
3 Wu Yiemin, Wang Longmei, DuTing. J Less-Common Met, 1985; 110: 187
4 杜挺,乐可襄.金属学报,1987;23:B203
5 乐可襄、杜挺.李继宗,沈汝美,金属学报,1987;23:A106
6 Sawyer J C, Wallace J F. Trans Am Foundrymen's Soc, 1968; 76: 386
7 Morrogh H. Trans Am Foundrymen's Soc, 1952; 60: 439
8 Breyer N. U S Pat, 1973: No. 3 726 669
9 Breyer N, Gordon P. In: The Microstructure and Design of Alloys, Proc 3rd Int Conf on the Strength of Metals and Alloys, Vol. 1, Combridge, Engl, 1973: 493
10 Elliott J F. Electr Furnace Conf Proc, 1974; 32: 62
11 日本铁钢协会.铁钢便览,I基础,第三版,东京:丸善株式会社,1981:23
12 Lupis C H P. Acta Metall, 1968; 16: 1365
13 吴夜明,杜挺.钢铁研究总院学报,1983;3:161
14 Sigworth G K, Elliott J F. Met Sci, 1974; 8. 298
15#12
No related articles found!
No Suggested Reading articles found!