Please wait a minute...
Acta Metall Sin  1988, Vol. 24 Issue (3): 242-247    DOI:
Current Issue | Archive | Adv Search |
INTERACTION BETWEEN C AND Sn IN Fe-C-Sn LIQUID SOLUTION
WANG Zhengyue;DU Ting;WANG Longmei Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing
Cite this article: 

WANG Zhengyue;DU Ting;WANG Longmei Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing. INTERACTION BETWEEN C AND Sn IN Fe-C-Sn LIQUID SOLUTION. Acta Metall Sin, 1988, 24(3): 242-247.

Download:  PDF(392KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The thermodynamic properties of Fe-C-Sn liquid solution have beenstudied by using the solubility method in the temperrature range 1300-1500℃ andby using the iso-tin-activity with silver bath at 1550℃. The results are summarizedas follows: 1. The relation between the solubility of C and the content of Sn in liquid Feare: 1300℃ [%C]_(sat)=4.65-0.086[%Sn] 1400℃ [%C]_(sat)=4.86-0.106[%Sn] 1500℃ [%C]_(sat)=5.13-0.131[%Sn] 2. The solubility of C dependence on the content of Sn and the temperature isobtained as [%C]_(sat)=8.41-0.101[%Sn]-5904(1/T) 3. The temperature dependence of interaction coefficients between Sn and C inC saturated liquid Fe are ε_C~(Sn)=-(27170)/T+20.07; e_(Sn)~C=-(51.29)/T+0.041 4. The temperature dependence of interaction coeffients between Sn and C inliquid Fe are derived as e_C~(Sn)=-(194)/T+0.151; e_(Sn)~C=-(1810)/T+1.39 5. The first and second order interaction coefficients between Sn and C in liq-uid Fe at 1550℃ are determined as e_(Sn)~C=0.12; e_C~(Sn)=0.016; γ_(Sn)~C=0
Key words:  Fe-C-Sn solution      C-Sn interaction      solubility method      iso-activity method     
Received:  18 March 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I3/242

1 魏寿昆.活度在冶金物理化学中的应用.北京:中国工业出版社,1964:90
2 Lupis C H P. Acta Metall, 1968; 16: 1365
3 吴夜明,杜挺.钢铁研究总院学报,1983:3:161
4 Sigworth G K, Elliott J F. Met Sci, 1974; 8: 298
5 Hanson H. Constitution of Binary Alloys. New York: McGraw-Hill 1958: 11,20
6 Koros P J, Chipman J. J Met, 1956; 8: 1102
7 齐国均,冀春霖,见:全国第五届冶金物理化学年会论文集,西安,1984:227
8 周继程,田彦文.见:全国第五届冶金物理化学年会论文集,西安,1984:119
9 盛利贞,小笠原武司,长谷川宏,(白田)山卓三,山田武弘.铁钢,1960;46:1147
10 不破祐,藤仓正国,的场幸雄.铁钢,1960;46:235
11 Neumann F, Hermann S. Arch Eisenhuettenwes, 1959; 30: 477W
[1] ZHOU Qianli;DU Ting Central Iron and Steel Research Institute. Ministry of Metallurgical Industry; Beijing. INTERACTION BETWEEN C AND Sb IN Fe-C-Sb LIQUID SOLUTION[J]. 金属学报, 1988, 24(6): 527-529.
No Suggested Reading articles found!