Please wait a minute...
Acta Metall Sin  1988, Vol. 24 Issue (2): 71-75    DOI:
Current Issue | Archive | Adv Search |
INTERNAL FRICTION ASSOCIATED WITH MARTENSITIC TRANSFORMATION OF ASCAST MANGANESE-COPPER ALLOYS
XIE Cunyi;WEN Yiting;ZHU Xianfang Institute of Solid State Physics; Academia Sinica; Hefei
Cite this article: 

XIE Cunyi;WEN Yiting;ZHU Xianfang Institute of Solid State Physics; Academia Sinica; Hefei. INTERNAL FRICTION ASSOCIATED WITH MARTENSITIC TRANSFORMATION OF ASCAST MANGANESE-COPPER ALLOYS. Acta Metall Sin, 1988, 24(2): 71-75.

Download:  PDF(369KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Internal friction of martensitic transformation of as-cast manga-nese-copper alloys with Mn-content 90% was studied. Results show that the peak tem-perature of the stable peak (T=0) at low frequencies is independent of the mea-suring frequency, but the peak height decreases with increasing frequency. It is,therefore, not of a static hysteresis mechanism. The peak height is dependent onT and f at a constant heating or cooling rate, but it does not show a linear rela-tionship with T, 1/f or T/f. The peak height is independent of the strain amplitudein the range (A_e: 1×10~(-5)-1×10~(-4)). Consequently the low frequency internal fric-tion of martensitic transformation is not only a volume effect, but also a surfaceeffect connected with coherent boundaries.
Key words:  manganese-copper alloy      internal friction of martensitic transformation      Delorme-Dejonghe's model      effect of volume and interface     
Received:  18 February 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I2/71

1 Sugimoto K, Mori T, Shiode S. J Mater Sci, 1973; 7: 103
2 王业宁,杨正举,祝和,马进超. 南京大学学报,1963;7:1
3 Delorme J F, Schmid R, Robin M. J Phys (Paris), 1971; 32: C2--101
4 Dejonghe W, de Batist R, Delacy L.Scr Metall, 1976; 10: 1125
5 Bidaux J E, Schaller R, Benoit W. J Phys(Paris), 1985; 46: C10--601
6 Wen Yiting, Xie Cunyi, Chen Hui. J Phys(Paris), 1985; 46: C10--413
7 Luo Laizhong, Zhang Jinxiu. J Phys(Paris), 1985; 46: C10--649
8 文亦汀,王力田,杜家驹.物理,1986; 15: 109
9 Mercier O, Melton K N, de Preville Y. Acta Metall. 1979; 27: 1467
10 杨照金,邹一峰,张志方,王业宁.金属学报,1982;18:21
11 马应良,葛庭燧.物理学报,1964;20:72
12 王业宁,邹一峰,张志方.物理学报,1980;29:153
No related articles found!
No Suggested Reading articles found!