| AN NMR STUDY OF HYDROGEN MOTION IN LaNi_5, LaNi_4Cu AND LaNi_4Fe LATTICES |
| ZHOU Daming Department of physics;Nankai University;Tianjin;HOU Lei;JIN Qinghua;GUO Zhenya;DING Datong Nankai University; Tianjin |
|
Cite this article:
ZHOU Daming Department of physics;Nankai University;Tianjin;HOU Lei;JIN Qinghua;GUO Zhenya;DING Datong Nankai University; Tianjin. AN NMR STUDY OF HYDROGEN MOTION IN LaNi_5, LaNi_4Cu AND LaNi_4Fe LATTICES. Acta Metall Sin, 1988, 24(2): 189-193.
|
|
|
Abstract The continuous wave NMR (nuclear magnetic resonance) results of ~1Hin LaNi_5·H_6, LaNi_4Cu·H_x and LaNi_4Fe·H_x were reported. The line shape at bothhigher and lower temperatures, the activation energy of diffusion, the self correla-tion time and the diffusion coefficient calculated according to a model have beendiscussed. It was concluded that the partial substitution of Cu and Fe for Ni increasesthe stability of hydrogen in the host alloy.
|
|
Received: 18 February 1988
|
1 Van Vucht J H N, Kuijpers F A, Bruning H C A M. Philips Res Rep, 1970; 25: 133 2 Van Mal H H. Buschow K H J, Miedema A R. J Less-Common Met, 1974; 35: 65 3 Halstead T K. J Solid State Chem, 1974; 11: 114 4 Barnes R S, Harper W C, Nelson S O, Thome D K. Torgeson D R. J Less-Common Met, 1976; 49:483 5 Karlicek R F Jr, Lowe I J. J Less-Common Met. 1980; 73: 219 6 Chang H, Lowe I J, Karlicek R F Jr. In: Kaufmann, Shenoy eds. Nuclear and Electron Resonance Spectroscopies Applied to Material Science, 1981: 7 Drain L E. Proc Phys Soc, 1962; 80: 1380 8 Bloembergen N, Purcell E M, Pound R V. Phys Rev. 1948; 73: 679 9 Weaver H T. J Cham Phys, 1972; 56: 3193 10 StalinsByk Coogan C K. Gutowsky H S. J Chem Phys, 1961; 34: 1191 11 Kubo R, Tomita K. J Phys Soc Jpn. 1954; 9: 888 12 侯磊.镧镍(铜、铁)氢合金的氢位及运动研究.硕士学位论文,南开大学物理系,1986年6月 13 Bowman R C Jr, Gruen D M. MendeIsohn M. H.. Solid State Commun, 1979; 32: 501 14 Bowman A L, Anderson J L, Nereson N G. In: Proc 10th Rare Earth Res Conf, Carefree, Arizona: 1972: 485 15 Percheron-Guegan A, Lartigue C, Achard J C, Germi P, Tasset F. J Less-Common Met, 1980; 74: 1 16 Yartys' V A. Burnasheva V V. Semenenko K N, Fadeeva N V. Solov'ev S P. J Hydrogen Energy, 1982; 7(12) : 957 17 Achard J C, Lart gue C, Percheron-Guegan A. J Less-Common Met. 1982; 88: 89 18 Richter D, Hempelmann R, Vinhas L A. J Less-Common Met, 1982; 88: 353 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|