Please wait a minute...
Acta Metall Sin  1987, Vol. 23 Issue (6): 553-559    DOI:
Current Issue | Archive | Adv Search |
Ce-O, Ce-S AND Ce-S-O EQUILIBRIA IN LIQUID Ni
by WANG Longmei; DU Ting (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) (Manuscript received 10 February; 1986; revised manuscript 11 August; 1986)
Cite this article: 

by WANG Longmei; DU Ting (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) (Manuscript received 10 February; 1986; revised manuscript 11 August; 1986). Ce-O, Ce-S AND Ce-S-O EQUILIBRIA IN LIQUID Ni. Acta Metall Sin, 1987, 23(6): 553-559.

Download:  PDF(425KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Reaction constants of the formation of Ce_2O_3, CeS and Ce_2O_2S in liquid Ni at 1500 to 1600℃ have been determined, then the standard Gibbs energies (J·mol) were obtained: △G°_(Ce_2O_3)=-116240+315.8 T △G°_(Ces)=-570280+220.1 T △G°_(Ce_2O_2S)=-984850+238.5 T The reaction coefficients e_O~(Ce) and e_S~(Ce) have also be determined: e_O~(Ce)=-333451/T+149.7 e_S~(Ce)=-276228/T+146.0 The equilibrium phase diagram of a_o-a_s for Ni-Ce-S-O system at 1600℃ was also given.
Received:  18 June 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I6/553

1 王龙妹,杜挺.金属学报,1984;20:A286
2 王龙妹,杜挺.金属学报,1985;21:A249
3 王龙妹,杜挺.中国稀土学报,198S;3(2) :76
4 Schmalzfried H. Z Electrochem Ber Bunsenges Gesell Phys Chem, 1962; 66: 572
5 Fischer W A, Ackerman W A, Arch Eisenhuettenwes, 1966; 37: 43
6 Janke D. Fischer W A. Arch Eisenhuettenwes, 1975; 46: 755
7 徐秀光,王常珍,张贺林.东北工学院学报,1983;37(4) :29
8 Wang Longmei, Du Ting. Proc of the Int Conf on Rare Earth Development and Applications, Beijing, 1985, Beijing: Science Press, 1985, Vol; Ⅱp. 1165
9 Buzek Z. Hutn Listy, 1979; 34(10) : 699
10 Venal W V, Geiger G H. Metall Trans, 1973; 4: 2567
11 Vahed A, Kay D A R. Metall Trans, 1976; 7B: 375
12 《数学手册》编写组.数学手册,人民教育出版社,1979:8
13 王龙妹,杜挺.稀土.1983;(4) :48
No related articles found!