| SOLUBILITY OF NIOBIUM CARBIDE IN A MICROALLOY STEEL |
| by ZHENG Lu; YONG Qilong; SUN Zhenbao (Central Iron and Steel Institute; Ministry of Metallurgical Industry; Beijing) (Manuscript received 29 September; 1985; revised manuscript 8 April 1986) |
|
Cite this article:
by ZHENG Lu; YONG Qilong; SUN Zhenbao (Central Iron and Steel Institute; Ministry of Metallurgical Industry; Beijing) (Manuscript received 29 September; 1985; revised manuscript 8 April 1986). SOLUBILITY OF NIOBIUM CARBIDE IN A MICROALLOY STEEL. Acta Metall Sin, 1987, 23(6): 547-552.
|
|
|
Abstract The solubility of niobium carbide in γ-Fe of a microalloy steel, in which the Nb/C ratio is approximately equal to the stoichimetrie ratio of the carbide, has been determined by means of electrolytic extraction: lg([Nb]·[C]~(0.875))_v=2.97—7500/T±0.06(850—1200℃) The solubilities of it in γ-Fe and α-Fe have also been derived using the latest thermodynamic data, following results were obtained: lg([Nb]·[C]~(0.875))_v=3.24—7150/T(1100—1600K) lg([Nb]·[C]~(0.875))_0=4.87—10060/T(300—1000K)
|
|
Received: 18 June 1987
|
1 Microalloying 75, Proc. of an Int. Symp. on High-Strength Low-Alloy Steel, New York; Union Carbide Corp., 1977 2 De Kazinczy F, Axans A, Pachleitner P. Jernkontorets Ann, 1963; 147: 408 3 小山伸二,石井辉雄,成田贵一.日本金属学会益,1971;35:698 4 盛利贞,时实正治,中嶋由行,佐伯俊秀。铁鋼,1965;51:2031 5 Irvine K J, Picketing F B, Gladman T. J Iron Steel Inst, London, 1967; 205: 161 6 Nordberg H, Aronsson B. J Iron Steel Inst, London, 1968; 206: 1263 7 Hudd R C, Jones A, Kale M N. J Iron Steel Inst, 1971; 209: 121 8 Narcta K. Trans Iron Steel Inst Jap, 1975; 15: 145 9 Lakshmanan V K, Kirkaldy J S. Metall Trans, 1984; 15A: 541 10 Sharma R C, Lakshmanan V K, Kirkaldy J S. Metall Trans, 1984; 15A: 545 11 雍岐龙,郑鲁.金属学报,1984;20:A9 12 雍岐龙,郑鲁,孙珍宝.金属学报,1986;22:A529 13 Chipman J. Metall Trans, 1972; 3: 55 14 Barin I, Dnacke O. Thermochemical Properties of Inorganic Substances, Berlin: Springer-Verlag. 1973, p, 116-118 15 Schenck H, Frohberg M G, Reinders F. Stahl Eisen, 1963; 83:93 16 Smith R P. Trans Metall Soc AIME, 1960; 224: 190 17 Hoogendoorn T M, Spanraft M J. Microailoying 75, Proc. of an Int. Symp, on High-Strength Low-Alloy Steel, New York: Union Carbide Corp., 1977, p. 7 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|