INITIATION OF MICROCRACKS IN WC-Co ALLOYS
by SONG Shihong; LI Jianchun (Central-South University of Technology) (Manuscript received 10 December 1985; revised manuscript 14 June; 1986)
Cite this article: 

by SONG Shihong; LI Jianchun (Central-South University of Technology) (Manuscript received 10 December 1985; revised manuscript 14 June; 1986). INITIATION OF MICROCRACKS IN WC-Co ALLOYS. Acta Metall Sin, 1987, 23(6): 521-526.

Download:  PDF(2048KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The initiation of microcracks and its connection with microstructure of WC-Co hardmetals have been studied by STEM. The microcracks in specimens are induced by high-frequency compressive fatigue. The causes of microcrack initiation are explained by traverse of slipping dislocations across sub-grain and WC/WC grain boundaries and the pile-up of dislocations near the boundaries. The reduction of substructure dimension is required to improve the alloy quality.
Received:  18 June 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I6/521

1 Suzuki H, Hayashi K. Trans Jpn Inst Met, 1975; 16: 353
2 Suzuki H, Tanase T. Planseeber Pulvermetall, 1976; 242: 71
3 Roebuck B, Almond E A. Recent Advances in Hardmetal Production(Proc. Conf.), Loughborough University of rech. and Metall Powder Report, Vol. 2, 1979: 28
4 Chermant J L, Osterstock F. J Mater Sci, 1976; 11: 1939
5 Engel U, Huebner H. J Mater Sci. 1978; 13: 2003
6 Johannesson T, Lehtinen B, Philos Mag, 1971; 24: 1079
7 Hagege S, Nouet G, Delavignette P. Phys Status Solidi(a), 1980; 61: 675
8 Chermant J L, Deschanvres A, Osterstock F. Powder Metall, 1977; 2: 63
9 Gurland J. Jernkontorets Ann, 1963; 4: 147
10 宋士泓,刘武,李健纯.理化检验,物理分册,1987;23(1) :28
11 Jayaram V, Sinclair R, Rowcliffe D J. Acta Metall, 1983; 31: 373
No related articles found!
No Suggested Reading articles found!