| DYNAMIC PROCESS OF MARTENSITIC STABILIZATION IN A Cu-Zn-Al ALLOY |
| by TAN Shusong; GAO Xiujuan (South-Central Polytechnic University) (Manuscript received 28 October; 1985; revised manuscript 18 July; 1986) |
|
Cite this article:
by TAN Shusong; GAO Xiujuan (South-Central Polytechnic University) (Manuscript received 28 October; 1985; revised manuscript 18 July; 1986). DYNAMIC PROCESS OF MARTENSITIC STABILIZATION IN A Cu-Zn-Al ALLOY. Acta Metall Sin, 1987, 23(6): 527-530.
|
|
|
Abstract The dynamic process of stabilization of thermoelastic martensite in a Cu-Zn-Al alloy has been studied by means of electro-resistance and X-ray diffraction. It was found that the structure of the sample quenched into cold water (
|
|
Received: 18 June 1987
|
1 谭树松,黄健超.中南矿冶学院学报,1984;(4) :19 2 祝向永,唐远永,曹明盛.中南矿冶学院学报,1981;(3) :1 3 Dunne D P, Kennon N F. Scr Metall, 1982; 16: 729 4 孔祥炎,高安娟.中南矿冶学院学报,1983;(2) :49 |