STUDY OF THE COARSE GRAINS OF QUENCHED LD2 ALLOY FORGING
by WU Baoshan (Lanzhou University); YU Zizun (Northwestern Aluminium Fabrication Factory; Lanzhou) (Manuscript received 18 April; 1985; revised manuscript 3 December; 1985)
Cite this article: 

by WU Baoshan (Lanzhou University); YU Zizun (Northwestern Aluminium Fabrication Factory; Lanzhou) (Manuscript received 18 April; 1985; revised manuscript 3 December; 1985). STUDY OF THE COARSE GRAINS OF QUENCHED LD2 ALLOY FORGING. Acta Metall Sin, 1987, 23(6): 507-513.

Download:  PDF(1469KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  In the past, coarse grains were often formed in the central part of LD2 alloy forging after quenching, that made many products waste. In this paper, a simulated test was planned to study the formation of coarse grains by means of X-ray diffraction and metallographic observation. Some technological factors which have influences to the formation of coarse grains, such as strain, deformation and quenching temperature, soaking time, etc. have been studied. The causes of coarse grains and their formation mechanismas well as the elimination of coarse grains have been discussed.
Received:  18 June 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I6/507

No related articles found!
No Suggested Reading articles found!