Abstract Solid solubilities of Ce and Nd in α-Fe were determined with the aid of X-ray diffraction lattice parameter measurements and electron-microprobe quantitative analysis. The alloys were prepared by vacuum levitation melting using 99.987wt-%Fe, 99.9wt-%Ce and 99.95wt-%Nd, respectively. They were subsequently homogenized at 1200℃, then cooled down to room temperature to achieve quasi-equilibrium conditions. Solubilities of 0.048 wt-%Ce and 0.055 wt-% Nd in α-Fe were obtained.
|
|
Received: 18 June 1987
|
1 Jepson J O, Duwez P. Trans ASM, 1955; 47: 543-553 2 Richerd J. Mem Sci Roy Metall, 1962; 59: 527 3 Haefling J F, Daane AH. In: Spedding F H, Daane A H eds., The Rare Earth, New York: Wiley, 1961: 280 4 #12 5 庄应烘,荣国器,唐晓峰.中国稀土学报,1983;1(1) :58-61 6 #12 7 Domagala R F, Rausch J J, Levinson D W. Trans ASM, 1961; 53: 137-155 8 颜玉新,章复中.稀有金属(季刊),1987;6(2) :131 9 #12 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|