Please wait a minute...
Acta Metall Sin  1987, Vol. 23 Issue (6): 498-502    DOI:
Current Issue | Archive | Adv Search |
INFLUENCE OF Sr AND Sb ON SOLIDIFICATION OF Al-Si ALLOYS
by WANG Yucong; HUANG Liangyu; ZHAI Chunquan; DING Wenjiang (Shanghai Jiaotong University) (Manuscript received 4 November; 1985; revised manuscript; 3 May; 1986)
Cite this article: 

by WANG Yucong; HUANG Liangyu; ZHAI Chunquan; DING Wenjiang (Shanghai Jiaotong University) (Manuscript received 4 November; 1985; revised manuscript; 3 May; 1986). INFLUENCE OF Sr AND Sb ON SOLIDIFICATION OF Al-Si ALLOYS. Acta Metall Sin, 1987, 23(6): 498-502.

Download:  PDF(430KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The influence of Sr and Sb on the solidification process of Al-Si alloys. was investigated by differential thermal analysis(DTA). The contact angles between the melt and silicon substrates were measured, and the interfacial energies were calculated. It was obtained that Sr and Sb in the melt raised the Al-Si eutectic nucleation temperature and retarded the eutectic crystallization. Sr and Sb in the melt had no thermodynamic tendeney to absorb on silieon crystals, which was contrary to the traditional point of view. But Sr and Sb might accumulate on silicon crystals and affect the growth of Al-Si eutectics because the partition coefficients were less than 1.
Received:  18 June 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I6/498

1 Day M G, Hellawell A. Proc Roy Soc, 1968; A305: 473
2 Jenkinson D C, Hogan L M. J Cryst Growth, 1975; 28: 171
3 朱培钺.陈熙琛,贾均,张宝书,刘贤功.哈尔滨工业大学科学研究报告,第155期,1979
4 神户博太郎主编,刘振海,朴东奎,吴庸烈译.热分析,北京;化学工业出版社,1982:11
5 Loehberg K, Pattanayak DR. Aluminium, 1976; 52: 368
6 黄良余,王玉琮,翟春泉,丁文江.金属学报,1986;22:A310
No related articles found!