LOW TEMPERATURE STRUCTURAL RELAXATION OF METALLIC GLASS (Fe_(55) Ni_(45))_(78)Si_8 B_(14)
by JIANG Fangxin; XU Yan; YANG Guobin; LI Yang; FU Qiunan (Beijing: University of Iron and Steel Technology)(Manuscript received 15 July; 1985; revised manuscript 26 March; 1986)
Cite this article: 

by JIANG Fangxin; XU Yan; YANG Guobin; LI Yang; FU Qiunan (Beijing: University of Iron and Steel Technology)(Manuscript received 15 July; 1985; revised manuscript 26 March; 1986). LOW TEMPERATURE STRUCTURAL RELAXATION OF METALLIC GLASS (Fe_(55) Ni_(45))_(78)Si_8 B_(14). Acta Metall Sin, 1987, 23(5): 495-497.

Download:  PDF(249KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Internal friction and modulus (especially the changes of it at the temperatures below 500K) for Fe-Ni base metallic glass have been studied during structural relaxation using a Bordoni-type system. The results show that the structural relaxation may consist of two steps: the low temperature (below 500K)structural relaxation governed by TSRO and the high temperature (above 500K) one governed by both CSRO and TSRO. The activation energy of low temperature structural relaxation is about 17 kJ/mol.
Received:  18 May 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I5/495

1 Egami T. Mater Res Bull, 1978; 13: 557
2 Morito N, Egami T. J Non-Cryst Solids, 1984; 61&62: 973
3 Morito N, Egami T. Acta Metall, 1984; 32: 603
4 Scott M G, Kursumovic A. Acta Metall, 1982; 30: 853
5 Van Den Beukel A, Van Der Zwaag S, Mulder A L. Acta Metall, 1984; 32: 1895
6 Bordoni P G. Nuovo Cimento, 1947; 4: 177
7 Nowick A S, Berry B S. Anelastic Relaxation in Crystalline Solids, New York: Academic Press, 1972: 621
8 Weisberg L R, Quimby S L. Phys Rev, 1958; 110: 338
No related articles found!
No Suggested Reading articles found!