| COMPUTER SIMULATION OF RAPID SOLIDIFICATION IN SELF-QUENCHING |
| by ZHANG Jingguo; CAI Xinxing; HUANG Weiji; YAN Shopping (Shanghai Iron and Steel Research Insitute); KE Jun (T. Ko)(Beijing University of Iron and Steel Technology)(Manuscript received 4 April; 1985) |
|
Cite this article:
by ZHANG Jingguo; CAI Xinxing; HUANG Weiji; YAN Shopping (Shanghai Iron and Steel Research Insitute); KE Jun (T. Ko)(Beijing University of Iron and Steel Technology)(Manuscript received 4 April; 1985). COMPUTER SIMULATION OF RAPID SOLIDIFICATION IN SELF-QUENCHING. Acta Metall Sin, 1987, 23(5): 474-479.
|
|
|
Abstract The computer simulation was made of the rapid solidification in self-quenching with the moving Gaussian source model. Results are in agreement with those calculated analytically and coincide with experimental values when v= 4.25-97.5cm/s. The computation can be performed with a microcomputer.
|
|
Received: 18 May 1987
|
1 Strutt P R. Mater Sci Eng, 1980; 44: 239 2 Greenwald L E, Breinan E M, Kear B H. AIP Conf Proc, 1979; (50) : 189 3 Matyja H, Giessen B C, Grant N J. J Inst Met, 1968; 96: 30 4 Klemens P G. J Appl Phys, 1976; 47: 2165~ |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|