| CALCULATION OF ACTIVITIES ON TWO-PHASE REGION BOUNDARIES IN CaO-Al_2 O_3 -SiO_2 TERNARY SYSTEM |
| by CAI Wenjuan; ZHOU Guozhi(Beijing University of Iron and Steel Technology)(Manuscript received 16 July; 1985; revised manuscript 14 May; 1986) |
|
Cite this article:
by CAI Wenjuan; ZHOU Guozhi(Beijing University of Iron and Steel Technology)(Manuscript received 16 July; 1985; revised manuscript 14 May; 1986). CALCULATION OF ACTIVITIES ON TWO-PHASE REGION BOUNDARIES IN CaO-Al_2 O_3 -SiO_2 TERNARY SYSTEM. Acta Metall Sin, 1987, 23(5): 480-485.
|
|
|
Abstract Calculation of activities on the two-phase region boundaries in CaO-Al_2O_3-SiO_2 ternary system has been carried out. Relationships between the activities of components and the composition of intersection of tie-line and composition edges along two-phase boundaries have also been presented, upon which the activities may easily be read. This method can also be used in other ternary systems.
|
|
Received: 18 May 1987
|
1 Chou K C(Zhou Guozhi) (周国治), Elliott J F. Chemical Metallurgy-A Tribute to Carl Wagner, New York: AIME, 1981: 195 2 周国治,蔡文娟,马美娟。见:第三届全国熔盐化学和电化学会议论文集,三元系中两相区边界上的活度之间的关系,1985 3 周国治,蔡文娟,马美娟.见:第三届全国熔盐化学和电化学会议论文集,三元系中两相区边界上的活度与t函数之间的关系,1985 4 Choudary U V, Chang Y A. Metall Trans, 1976; 7B: 655 5 Wang Zhichang (王之昌), Zhou Guozhi (周国治), Scientia Sinica, 1984; 27(12) : 1328-1338 6 Zhou Guozhi (周国治). Scientia Sinica, 1978; 21(5) : 601 7 Elliott J F, Gleiser M, Ramakrishna V. Thermochemistry for Steelmaking, Vol. Ⅱ, Reading Mass: Addison-Wesley, 1963: 592-59 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|