Please wait a minute...
Acta Metall Sin  1987, Vol. 23 Issue (5): 459-463    DOI:
Current Issue | Archive | Adv Search |
MAGNETIC PROPERTIES AND RELAXATION PROCESS OF AMORPHOUS CoFeNiNbSiB SOFT MAGNETIC FILMS
by LIU Yihua; MEI Liangmo; WANG Dexin; GUO Yicheng (Department of physics; Shandong University; Jinan)(Manuscript received 10 July; 1985; revised manuscript 10 January; 1986)
Cite this article: 

by LIU Yihua; MEI Liangmo; WANG Dexin; GUO Yicheng (Department of physics; Shandong University; Jinan)(Manuscript received 10 July; 1985; revised manuscript 10 January; 1986). MAGNETIC PROPERTIES AND RELAXATION PROCESS OF AMORPHOUS CoFeNiNbSiB SOFT MAGNETIC FILMS. Acta Metall Sin, 1987, 23(5): 459-463.

Download:  PDF(440KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The preparing processes of amorphous CoFeNiNbSiB soft magnetic thin films using r. f. sputtering have been investigated systematically. It was found that high quality soft magnetic films can be obtained at low pressure Ar(0.5 Pa), and the properties of films are less influenced by the bias. After annealing in a rotating field, the initial permeability of films is not less than 3000, at the field up to 10 MHz, and they show a good frequency response! The structural relaxation process of amorphous films during annealing has been studied by means of resistance monitoring method. Four successive relaxation stages have been observed at high temperature.
Received:  18 May 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I5/459

1 Shimada Y, Hasegawa T, Kojima H. IEEE Trans Magn, 1981; MAG-17: 1199
2 Sakakima H. IEEE Trans Magn, 1983; MAG-19: 131
3 Fujimori H, Kazama N S, Hirose K, Zhang Jiaji, Morita H, Sato I, Sugawara H. J Appl Phys, 1984; 55 (6) : 1769
4 刘玉志,刘光棣,朱祥宾,李长才,张秋荣,陈炜.上海钢研(专辑)。冶金部首届非晶态合金及应用学术交流会论文集,上海钢铁研究所,1983:9
5 刘宜华,栾开政,郭贻诚.科学通报,1984;29(23) :1419
6 Kajiura M, Togami Y, Kobayashi K, Teranishi T. Jpn J Appl Phys, 1981; 20 (6) : L389
7 Hoshi Y, Kazama H, Naoe M, Yamanaka S. IEEE Trans Magn, 1983; MAG-19: 1958
8 Wasede Y, Okazaki H, Masumoto T. J Mater Sci, 1977; 12: 1927
No related articles found!