EFFECT OF CONCENTRATION AND TRANSITION METALS ON CRYSTALLIZATION OF Fe-BASED AMORPHOUS ALLOYS
by SHEN Baogen; ZHAN Wenshan; ZHAO Jiangao; CHEN Jinchang;PAN Xiaoshuo (Institute of Physucs; Academia Sinica; Beijing)(Manuscript received 28 January; 1985; revised manuscript 12 November; 1985)
Cite this article: 

by SHEN Baogen; ZHAN Wenshan; ZHAO Jiangao; CHEN Jinchang;PAN Xiaoshuo (Institute of Physucs; Academia Sinica; Beijing)(Manuscript received 28 January; 1985; revised manuscript 12 November; 1985). EFFECT OF CONCENTRATION AND TRANSITION METALS ON CRYSTALLIZATION OF Fe-BASED AMORPHOUS ALLOYS. Acta Metall Sin, 1987, 23(5): 452-458.

Download:  PDF(552KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The crystallization kinetics studies during the recent years on the FeB and FeCoBSi Series of amorphous alloys as well as on the effect of alloying with various transition metals are summarized. The specimens were ribbons of 30—50 μm thickness and 1—2μm width prepared by the melt quenching technique. DSC and thermomagnetic measurements, and sometimes X-ray diffraction investigations were carried out. The main results are: (1) for the Fe_(100-x)B_x series, both the incipient crystallization temperature, T_(cr), and the corresponding activation energy, △E, exhibit a maximum value at x=16; (2) when the alloy composition was varied or an alloying transition element was added, both T_(cr) and △E increased with decreasing average number outer electrons per atom which was calculated by taking into account both the s, p and d electrons of the transition metal atoms. These and other less significant results are discussed in connection with various factors commonly regarded as effecting the stability of amorphous alloys.
Received:  18 May 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I5/452

1 Naka M, Masumoto T. Sci Rep Res Inst Tohoku Uni, 1979; 27A(2) : 118
2 Donald I W, Davies H A. In: Cantor B ed., Rapidly Quenched Metals III, Vol. 1, London: The Metals Society, 1978: 273
3 Donald I W, Ward K D, Davies H A, Crangle J. In: Masumot T, Suzuki K eds.. Rapidly Quenched Metals IV, Vol. 1, Sendai: Japan Inst Met, 1981: 597
4 Kissinger H E. J Res Nat Bur Stand, 1956; 57: 217 Kissinger H E. Analy Chem, 1957; 29: 1703 Luborsky F E, Liebermann H H. Appl Phys Lett, 1978; 33: 233
5 Matsuura M. Solid State Commun, 1979; 30: 231
6 Chen H S. Appl Phys Lett, 1976; 29: 12
7 Zhan W S (詹文山), Shen B G(沈保根), Luo H Y(罗海英), Yu B L (俞伯良).In: Masumoto T, Suzuki K eds., Rapidly Quenched Metals IV, Vol. 2, Sendai: Japan Inst Met, 1981: 1137
8 陈金昌,司红,沈保根,詹文山,赵见高.金属学报,1985:21:B140
9 Naka M, Tomizawa S, Masumoto T, Watanabe T. In: Grant N J, Giessen B. C eds., Raoidly Quenched Metals II, USA: MIT, 1976
10 Chen H S. Acta Metall, 1976; 24: 153
11 Waseda Y, Chen H S. Sci Rep Res Inst Tohoku Uni, 1980; 28A(2) : 143
12 Zhao J G (赵见高), Shen B G (沈保根), Zhan W S (詹文山), Chen JC(陈金昌),J Magn Magn Mater, 50(1985) ,11
No related articles found!
No Suggested Reading articles found!