Please wait a minute...
Acta Metall Sin  1987, Vol. 23 Issue (5): 369-373    DOI:
Current Issue | Archive | Adv Search |
STRUCTURE AND TEMPER EMBRITTLEMENT OF LARGE SECTION 5Cr2NiMoVSi HOT-WORK DIE
by HU Xiang; LIN Yansheng; HUANG Zheng'an; .FENG Ganjfang; XU Yuxian (Huazhong University of Science and Technology; Wuhan)(Manuscript received 16 March; 1985; revised manuscript 17 July; 1985)
Cite this article: 

by HU Xiang; LIN Yansheng; HUANG Zheng'an; .FENG Ganjfang; XU Yuxian (Huazhong University of Science and Technology; Wuhan)(Manuscript received 16 March; 1985; revised manuscript 17 July; 1985). STRUCTURE AND TEMPER EMBRITTLEMENT OF LARGE SECTION 5Cr2NiMoVSi HOT-WORK DIE. Acta Metall Sin, 1987, 23(5): 369-373.

Download:  PDF(1156KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  To investigate the structure of quenched and tempered large section die, the cooling rate simulating that of central part for 300×300mm section has been used during quenching. As a comparision, ordinary quenching process has also been carried out. TEM observation shows that the structure of the latter is mainly lath martensite, and that of the former is B_I -bainite, which possesses higher temper stability than those found in low carbon low alloy steels. Transforming of great quantity of retain austenite and creating of chain-like distributed M_3C are considered as the main reason of the embrittement for the large section dies.
Received:  18 May 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I5/369

1 范雄主编.X射线金属学,机械工业出版社,1981
2 Bhadeshia H K D H, Edmonds D V. Metall Trans, 1979; 10A: 895
3 Huang Der-Hung, Thomas G. Metall Trans, 1977; 8A: 1661
4 大森靖也,大谷泰夫,邦武立郎.铁钢,1971;57:1690
5 #1