C-C INTERACTION ENERGY IN Fe-C ALLOYS
by MOU Yiwen; XU Zuyao (T. Y. Hsu) (Shanghai Jiaotong University) (Manuscript received 17 February; 1985)
Cite this article: 

by MOU Yiwen; XU Zuyao (T. Y. Hsu) (Shanghai Jiaotong University) (Manuscript received 17 February; 1985). C-C INTERACTION ENERGY IN Fe-C ALLOYS. Acta Metall Sin, 1987, 23(4): 329-338.

Download:  PDF(687KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A new approach has been suggested for the determination of the C-C interaction energy, the partial molar enthalpy and nonconfigurational entropy of carbon in the Fe-C austenite and ferrite from available activity data. By application of the values obtained through the approach to the calculation of the Fe-C phase diagram, the results in the equilibrium region are in very good agreement with the experimental one. From the scattered and limited experimental activity data, the C-C interaction energy obtained through the present approach should be more reasonable than that through previous efforts. Further analysis indicates, however, that up to now the activity data on carbon in ferrite are not accurate enough for obtaining the C-C interaction energy in ferrite with the clear physical significance.
Received:  18 April 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I4/329

1 Kaufman L, Radcliffe S V, Cohen M. In: Zackay V F, Aaronson H I, eds. Decomposition of Austenite by Diffusional Processes, New York: Interscience, 1962:313-352
2 Lacher J R. Proc Cambridge Philos Soc. 1937; 33:518
3 Fowler R H. Guggenheim E A. Statistical Thermodynamics, New York: Cambridge Univ. Press, 1939:442
4 McLellan R B, Dunn W W. J Phys Chem Solids, 1969; 30: 2631
5 Aaronson H I, Domian H A, Pound G M. Trans Metall Soc AIME, 1966; 236:753
6 Smith R P. J Am Chem Soc 1946; 68:1163
7 Shiflet G J, Bradley J R, Aaronson H I. Metall Trans 1978; 9A:999
8 Bhadeshia H D K H. Met Sci, 1980; 14:230
9 Lobo J A, Geiger G H. Metall Trans, 1976; 7A: 1347
10 Bhadeshia H D K H. Met Sci, 1982; 16: 167
11 Christian J W. Theory of Transformations in Metals and Alloys, Oxford: Pargamon, 1975:383
12 Kaufman L, Clougherty E V, Weiss R J. Acta Metall 1963; 11:323
13 Hsu T Y(Xu Zuyao), Mou Yiwen. Acta Metall, 1984; 32:1469
14 Lobo J A, Geiger G H. Metall Trans, 1976; 7A: 1359
15 Metals Handbook, Vol. 8,8th ed. Metal Park, Ohio: ASM, 1973:275
16 Shiflet G J, Bradley J R, Aaronson H I, Metall Trans, 1984; 15A: 1287
17 Bhadeshia H D K H. Acta Metall, 1980; 28:1265
18 Bhadeshia H D K H, Met Sci, 1981;15:178
No related articles found!
No Suggested Reading articles found!