THE CRITICAL STRESS OF FATIGUE CRACK INITIATION FOR MEDIUM CARBON STEEL |
by LIN Jizhong; LIU Shuhua; WU Yushu; LI Yi (China Academy of Railway Sciences) (Manuscript received 22 April; 1986; revised manuscript 25 August; 1986) |
|
Cite this article:
by LIN Jizhong; LIU Shuhua; WU Yushu; LI Yi (China Academy of Railway Sciences) (Manuscript received 22 April; 1986; revised manuscript 25 August; 1986). THE CRITICAL STRESS OF FATIGUE CRACK INITIATION FOR MEDIUM CARBON STEEL. Acta Metall Sin, 1987, 23(4): 339-340.
|
Abstract Notch fracture machanics was used to investigate the fatigue crack initiation from the notch tip for medium carbon steels (0.4-0.6 wt-%C). The relationships between the maximum stress range at the notch root, △σ_(max), and the number of cycles before fatigue crack initiation, N_i, have been determined. Furthermore, the threshold stress of fatigue crack initiation, △σ_(max)th, as a function of C content or of yield strength of the steel has been proposed.
|
Received: 18 April 1987
|
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|