LOW-ANGLE BOUNDARIES AND SUB-BOUNDARIES IN Al WITH CONVERGENT BEAM ELECTRON DIFFRACTION
by BIAN Weimin (Northeast Institute of Technology; Shenyang) (Manuscript received 21 February; 1986; revised manuscript 31 July; 1986)
Cite this article: 

by BIAN Weimin (Northeast Institute of Technology; Shenyang) (Manuscript received 21 February; 1986; revised manuscript 31 July; 1986). LOW-ANGLE BOUNDARIES AND SUB-BOUNDARIES IN Al WITH CONVERGENT BEAM ELECTRON DIFFRACTION. Acta Metall Sin, 1987, 23(4): 262-395.

Download:  PDF(3113KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A method has been advanced to determine precisely the orientation difference of the crystals between low-angle boundaries and sub-boundaries of high purity Al by convergent beam electron diffraction studies. The results show that the ones of low-angle and sub-boundaries are 1.55±0.051° and 0.32+0.037° respectively, as well as the curved angle of the crystal by single edge dislocation is 0.22±0.036°. The accuracy and error of the method have been analysed. Some problems concerning their structure of dislocation network and type were also discussed.
Received:  18 April 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I4/262

1 Spencer J P, Humphreys C J, Hirsch P B. Philos Mag, 1972; 26: 193