Abstract The attachment energy and specific surface energy of important faces of a ZrAl_3 crystal have been calculated by computer using the periodic bond chain method and the Lennard-Jones n-m potential parameters. The equilibrium form and growth form of the crystal have been deduced, and the theoretical growth form has been compared with the actual growth form observed in a melt growth experiment.
|
|
Received: 18 April 1987
|
1 Hartman P, Perdok W G. Acta Crystallogr. 1955; 8: 49, 521 2 Hartman P. In:Hartman P ed., Structure and Morphology in Crystal Growth: An Introduction, Amsterdam: North-Holland, 1973; 367 3 Felius R O. Structure morphology of Rutile and Trirutile Type Crystals, Dutch Efficiency Bureau, Pijnacker, 1976 4 Hartman P. J Cryst Growth, 1968; 2: 385 5 Hartman P, Bennema P. J Cryst Growth, 1980; 49: 145 6 Hartman P.J Cryst Growth, 1980; 49: 157, 166 7 Tassoni D, Riquet J P, Durand F. Acta Crystallogr, A, 1980; 36: 420 8 Hamer R, Tassoni D, Riquet J P, Durand F. J Cryst Growth, 1981; 51: 493 9 Brauer G. Z Anorg Allg Chem, 1939; 242: 1 10 Shu Zhen, Davies G J. J Cryst Growth, 1983; 64: 407 11 Fink W L, Willey L A. Trans AIME, 1939; 133: 69 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|