Please wait a minute...
Acta Metall Sin  1987, Vol. 23 Issue (3): 262-270    DOI:
Current Issue | Archive | Adv Search |
MASS-TRANSFER MODEL ANALYSIS OF ESR PROCESS ON INDUSTRIAL UNIT
WEI Jihe (Xi′an Institute of Metallurgy and Construction Engineering) MITCHELL A. (University of British Columbia; Vancouver; B. C.; Canada) (Manuscript received 17 September; 1984; revised manuscript 10 June; 1986)
Cite this article: 

WEI Jihe (Xi′an Institute of Metallurgy and Construction Engineering) MITCHELL A. (University of British Columbia; Vancouver; B. C.; Canada) (Manuscript received 17 September; 1984; revised manuscript 10 June; 1986). MASS-TRANSFER MODEL ANALYSIS OF ESR PROCESS ON INDUSTRIAL UNIT. Acta Metall Sin, 1987, 23(3): 262-270.

Download:  PDF(823KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The new model developed by the authors is used to predict and simulate the ingot and slag composition during the ESR process of Cr-Mo-V turbine rotor steel on an industrial unit. The results are shown to be in excellent agreement with those of practical process in an ingot diameter of 2300mm, also to agree with observations on Ca and Al deoxidation, and the model may be expected to offer a practical basis for the control of Composition during the ESR.
Received:  18 March 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I3/262

1 Wei Chiho (魏季和), Mitchell A. Proc. 3rd Process Technology Conf., AIME, Pittsburgh, March. 1982: 232
2 魏季和,Mitchcll A.全国第一届冶金反应动力学、第二届炼钢理论学术讨论会论文集(下),中国金属学会冶金物理化学学术委员会、炼钢学术委员会,1982:159
3 魏季和,Mitchell A.金属学报,1984;20:B261
4 Wei Chiho (魏季和), Mitchell A. Proc. 7th ICVM, ISIJ, Tokyo, Jpn, Nov. 1982: 1224
5#12
6 魏季和, Mitchell A. 金属学报, 1984; 20: B280
7 Jauch R, Choudhury A, Tince F, Lemor W R. Ironmaking Steelmaking, 1979; 6(2) : 75
8 Choudhury A, Jauch R, Tince F. Stahl Eisen, 1980; 100: 1012
9 Choudhury A, Jauch R, Tince F. Proc. 6th ICVM, Am. Vacuum Soc., San Diego, California, USA, April, 1979
10 Schwerdtfeger K, Wepner W, Pateisky G. Ironmaking Steelmaking, 1978; 5(3) : 135
11 Paton B E, Demchenko V F, Emelyanenko Yu G, Kozlitin D A et al. In: Paton B E ed, Proc. Conf. on Special Electrometallurgy, Part 1, Kiev, 1972: 144
12 Paton B E, Medovar B I, Kozlitin D A, Emel'yanenko YuG, et at. Electroslag Refining, ISI, London, 1973; 16
13 Etienne M, Ph. D. Thesis, University of British Columbia, 1970
14 Fraser M E, Mitchell A. Ironmaking Steelmaking, 1976; 3(5) 279; 288
15 Fraser M E. Ph. D. Thesis, University of British Columbia, 1974
16 Kamensky Yu M, Afanasjev YI, Sukhotin BN, Vegman E et al. In: Paton B. E. ed, Proc. Conf on Special Electrometallurgy, Part 1, Kiev, 1972: 33
17 Mitchell A, Jackson R O, Ballantyne A S. Proc. 4th Int. Symp. on ESR Processes, Tokyo, Jpn, 1973: 1
18 Mitchell A, Carmona F R, Wei Chiho (魏季和). Iron Steelmaker, 1982; 9(3) : 37
No related articles found!