| ELECTRODE PROCESS OF ELECTROLYTIC COATING OF Al IN FUSED NaCl-KCl SALT BATH |
| MA Zhangyuan; XU Zhiqiang; CAO Tieliang; SHI Shengtai (Shih Shing-Tai)(Shanghai Institute of Metallurgy; Academis Sinica) (Manuscript received 22 July; 1984; revised manuscript 26 November; 1985) |
|
Cite this article:
MA Zhangyuan; XU Zhiqiang; CAO Tieliang; SHI Shengtai (Shih Shing-Tai)(Shanghai Institute of Metallurgy; Academis Sinica) (Manuscript received 22 July; 1984; revised manuscript 26 November; 1985). ELECTRODE PROCESS OF ELECTROLYTIC COATING OF Al IN FUSED NaCl-KCl SALT BATH. Acta Metall Sin, 1987, 23(3): 257-261.
|
|
|
Abstract The standard oxidation/reduction potential of Al including its valence state in fused salt was examined, The anodic dissolution of Al can be shown by the equation Al→Al~3+3e. The standard oxidation/reduction potential of Al in fused salt is-1.122V as obtained by graphical method. Cathodic process has been investigated by means of steady state method. Separate potentials of some ions, the coefficient of diffusion ,of AlCl_4~- ion and kinetic constants of Al ion reduction have been meastured and discussed.
|
|
Received: 18 March 1987
|
1 石声泰 (Shin S T). In: Rapp R A ed., High Temperature Corrosion, NACE-6, 1983: 460 2 石声泰.中国腐蚀与防护学报,1981;1(3) :1-7 3 石声泰,冯明仁,曹铁梁,马樟源,张彩玲.中国腐蚀与防护学报,1981;1(4) :1-7 4 Shin S T (石声泰), Feng M R (冯明仁), Cao T L (曹铁梁), Zhang C L (张彩玲). In: Metallic Corrosion, Proceedings 8th International Congress on Metallic Corrosion, 1981, Vol. Ⅱ, Deutsche Gesellschaft fur Chemisches Apparalewesen e. v. Frankfurt am Main, 1981: 1127 5 Winter D G, Strachan A M. In: Jones M J. Advances in Extractive Metallurgy, An Int. Symp. Organized by the Institution Metallurgy, London: Inst. Mining and Metall., 1977: 177 |