PHASE EQUILIBRIA IN Al-Mg-Sm SYSTEM AT 400℃
ZHENG Chaogui; CHEN Lichong; YE Yupu (Department of Chemistry; Peking University) (Manuscript received 15 July; 1985; revised manuscript 26 May. 1986)
Cite this article: 

ZHENG Chaogui; CHEN Lichong; YE Yupu (Department of Chemistry; Peking University) (Manuscript received 15 July; 1985; revised manuscript 26 May. 1986). PHASE EQUILIBRIA IN Al-Mg-Sm SYSTEM AT 400℃. Acta Metall Sin, 1987, 23(3): 253-256.

Download:  PDF(309KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Phase equilibria in Al-Mg-Sm system at 400℃ have been investigated by means of microstrueture and chemical analysis as well as X-ray powder diffraction techniques. 15 single-phase regions, 27 two-phase regions and 13 threephase regions were found in this system. The microstructural observations show that the solubilities of Sm in Mg_5Al_8 and Mg_(17)Al_(12) are less than 0.5 and 1.0 wt-% respectively. No evidence of new phase has been observed in the system.
Received:  18 March 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I3/253

1 Hansen M. Constitution of Binary Alloys, New Work: McGraw-Hill, 2nd Edition, 1958: 106
2 Iandelli A. National Physical Laboratory Symposium No. 9: The Physical Chemistry of Metallic Solution and Intermetallic Compounds, Vol. 1, London: Her Majesty's Stationary Office, 1959: 369-379
3 #12
4 郑朝贵,陈立翀,田曙坚,叶于浦.无机化学,1986;2(2) :80
5 Buschow K H J. J Less-Common Met, 1971; 24: 117
6 Buschow K H J. J Less-Common Met, 1965; 8: 75
7 Buschow K H J. Philips Res Rep, 1965; 20(1) : 15
8 Mondolfo L F. Aluminum Alloys: Structure and Properties, London-Boston, Butterworths, 1976; 376
9 Castcels F J. J Less-Common Met, 1967; 13: 370
10 郑朝贵,洪学韵,钱久信,叶于浦.中国稀土学报.1984;1(2) :78
11 #12
12 #12
13 #12
14 郑朝贵,吴有余,钱久信,叶于浦.金属学报,1986;22(2) :B638
No related articles found!
No Suggested Reading articles found!