SLIP DEFORMATION AND FRACTURE OF DIRECTIONALLY SOLIDIFIED DZ-38G SUPERALLOY
YIN Wanquan; GAO Wei; ZHU Guiqiu; HU Zhuangqi (Institute of Metal Research; Academia Sinica; Shenyang) (Manuscript received 3 December. 1985; revised manuscript 11 June; 1986)
Cite this article: 

YIN Wanquan; GAO Wei; ZHU Guiqiu; HU Zhuangqi (Institute of Metal Research; Academia Sinica; Shenyang) (Manuscript received 3 December. 1985; revised manuscript 11 June; 1986). SLIP DEFORMATION AND FRACTURE OF DIRECTIONALLY SOLIDIFIED DZ-38G SUPERALLOY. Acta Metall Sin, 1987, 23(3): 243-316.

Download:  PDF(2808KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Directionally solidified DZ-38G superalloy was in situ observed under SEM in order to obtain a better understanding of its slip deformation and fracture process. The slips initiate in matrix and eutectic, and they are able to be transmitted by the eutectic. The slips on dendrite arms are much obvious than those in the interdendritic areas. The slip direction may slightly alter with the change of columnar grain orientation. The microcracks are prone to initiate at transverse grain boundarie, carbides on grain boundaries or eutectic/matrix interfaces. A microcrack usually propagates along a zig-zag path, and it is controlled by the maximum shear stress and tensile stress. The propagation of cracks is closely related to the straightness of columnar grain boundaries.
Received:  18 March 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I3/243

1 徐永波,穆在勤,刘民治,杨淑华.科学通报,1981:26:1356
2 Yin Wanquan (尹万全), Su Huihe (苏会和), Tong Yingjie (佟英傑), Liu Minzhi (刘民治). Int. Syrup. on Microstructure and Mechani cal Behaviour of Materials, Oct. 1985, Xi'an, China, Sponsored by Xi'an Jiaotong University, 1985; 29
3 林栋梁,黄颂惠.材料科学与工程,1985;(1) :4
No related articles found!
No Suggested Reading articles found!