Please wait a minute...
Acta Metall Sin  1987, Vol. 23 Issue (3): 240-242    DOI:
Current Issue | Archive | Adv Search |
RECRYSTALLIZATION IN Ti-10V-2Fe-3Al ALLOY
HU Dawei (Beijing Institute of Aeronautical Materials); PAN Yaqin; WU Yunshu (Beijing Institute of Aeronautics and Astronautics) (Manuscript received 23 October; 1985; revised manuscript 18 August; 1986)
Cite this article: 

HU Dawei (Beijing Institute of Aeronautical Materials); PAN Yaqin; WU Yunshu (Beijing Institute of Aeronautics and Astronautics) (Manuscript received 23 October; 1985; revised manuscript 18 August; 1986). RECRYSTALLIZATION IN Ti-10V-2Fe-3Al ALLOY. Acta Metall Sin, 1987, 23(3): 240-242.

Download:  PDF(564KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effect of hot deformation conditions on the recrystallization in Ti-10V-2Fe-3Al alloy was investigated. The working softening during deformation above T_β is due to the dynamic recovery. The recrystallization was considered as the static recrystallization following hot deformation. The volume fraction of recrystallzation decreases with increasing the deformation temperature. It is the temperature that causes the change of the β grain size prior to deformation. High strain rate will prompt the recrystallization.
Received:  18 March 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I3/240

1 庞丽频.北京航空学院毕业论文,1984
2 胡大为.北京航空学院硕士学位论文,1985
3 Semiatin S L, Lahoti G D. Metall Trans A, 1981; 12: 1709
4 胡大为,潘雅芩.航空用钛合金学术讨沦会,中国航空学会,宁波,1985年9月
5 Graham D. Diffusion in B. C. C. Metals, ASM Metals Park, Ohio, 1965, 2
No related articles found!