| EFFECT OF Ti ON PRECIPITATION AND MICROSTRUCTURAL PARAMETERS OF AN Al-Zn-Mg ALLOY |
| LIN Zhaoqi; ZHAO Gang (Northeast Institute of Technology; Shenyang) (Manuscript received 1 August; 1985) |
|
Cite this article:
LIN Zhaoqi; ZHAO Gang (Northeast Institute of Technology; Shenyang) (Manuscript received 1 August; 1985). EFFECT OF Ti ON PRECIPITATION AND MICROSTRUCTURAL PARAMETERS OF AN Al-Zn-Mg ALLOY. Acta Metall Sin, 1987, 23(2): 129-241.
|
|
|
Abstract The effect of an additive of 0.15 wt-% Ti in the Al-5.0Zn-1.8Mg alloy upon the precipitation, critical nucleation temperature, T'_c, and structural parameters has been investigated by means of hardness test as well as optical and TEM observations. The results showed that a trace additive of Ti may impel considerably the refinement of the grains of the alloy, but no more inhibition of its recrystallization and increase of T'_c.Ti may retard the growth of MPt, increase the density and the hardness of the alloy under lower temperature aging, namely, T_a T'_c. Furthermore, at any aging temperature between 120-200℃, the GBP and PFZ of the Ti-containing alloy are always finer and narrower than that of one free from Ti. It seems to be explained that influence of Ti addition on the precipitation and structural parameters would be caused by the participation of the Ti atom clusters in the nucleation of GP zone and the low concentration of excess vacancies in the Ti-containing alloy.
|
|
Received: 18 February 1987
|
1 杉山貞彦,福井利安.溶接学会誌,1966;35(11) :70 2 Mondolfo L F. Met Mater 1971; 5(6) : 207 3 Hernaez J, Madronero A. Weld J 1972; 51(6) : 281 4 Mudrack K P. Schweissen+Schneiden 1960; 12(2) : 45 5 馬場義雄,日本金属学会誌,1967;31:507 6 馬場義雄,日本金属学会誌,1967;31:513 7 馬場義雄,轻金属,1974;24:547 8 Grove C A, Judd G.Metall Trans 1973; 4: 1023 9 Chen C, Judd G. Metall Trans 1978; 9A: 553 10 林肇琦,封冰,孙贵经,杨胜坤.金属学报,1983;19:A197 11 林肇琦,朱及良,孙贵经,杨胜坤.金属学报,1984;20:A54 12 林肇琦,孙贵经,胡维平,杨胜坤.金属学报,1985;21:A119 13 林肇琦,赵刚,孙贵经,杨胜坤.金属学报,1985;21:A419 14 Embury J D, Nicholson R B. Acta Metall 1965; 13: 403 15 Noble B. Acta Metall 1968; 16: 393 16 Holl H A. J Inst Met 1964/65; 93: 364 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|