A STOCHASTIC MATHEMATICAL MODEL OF DECARBONIZATION KINETICS
QU Ying QIN Mingda DU Cainan (Beijing University of Iron and Steel Technology)
Cite this article: 

QU Ying QIN Mingda DU Cainan (Beijing University of Iron and Steel Technology). A STOCHASTIC MATHEMATICAL MODEL OF DECARBONIZATION KINETICS. Acta Metall Sin, 1987, 23(1): 82-85.

Download:  PDF(307KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A mathematical model is proposed and solved for the after-decarbonization at a range of low carbon using the stochastic differential equation.Certain statisti- cal parameters of the solution process have been calculated and discussed.The reliability of the model is verified by experimental data taking the volumetric mass transfer coefficient to be a constant.The application of the model to con- trol the after-decarbonization of converter process is studied considering an exten- sion of the volumetric mass transfer coefficient into general stochastic parame- ter.
Received:  18 January 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I1/82

1 杜才难.北京钢铁学院学报,1984;(1) :190
2 秦明达.北京钢铁学院学报,1982;(4) :89
3 秦明达.曲英,冶金反应动力学及第二届炼钢理论学术讨论会论文集(上册),1982年4月,重庆,199
4 Soong T T,Random Differential Equations in Science and Engineering,New York:Academic Press,1973,127
5 秦明达,杜才难.北京钢铁学院学报,1984;(2) :131+
No related articles found!
No Suggested Reading articles found!