PREDICTION OF THERMODYNAMIC FUNCTIONS OF BINARY OXIDES OF HIGH TEMPERATURE FOR INORGANIC THERMODYNAMIC CHEMISTRY DATABASE
by ZHU Jianzhong CHEN Bin XU Hua CHEN Nianyi (Shanghai Institute of Metallurgy;Academia Sinica);WANG Leshan XU Zhihong (Institute of Chemical Metallurgy;Academia Sinica;Beijing)
Cite this article: 

by ZHU Jianzhong CHEN Bin XU Hua CHEN Nianyi (Shanghai Institute of Metallurgy;Academia Sinica);WANG Leshan XU Zhihong (Institute of Chemical Metallurgy;Academia Sinica;Beijing). PREDICTION OF THERMODYNAMIC FUNCTIONS OF BINARY OXIDES OF HIGH TEMPERATURE FOR INORGANIC THERMODYNAMIC CHEMISTRY DATABASE. Acta Metall Sin, 1987, 23(1): 57-62.

Download:  PDF(477KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Mathematical models for estimating thermodynamic functions of binary oxi- des at high temperature have been developed.According to these models,values of four thermodynamic functions of some compounds at different temperatures have been predicted.Root mean square errors of them are of same order of the experimental errors.
Received:  18 January 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I1/57

1 许志宏,王乐珊,化工冶金,1980;5:88
2 Latimer W M,J Am Chem.Soc,1951;73:1480
3 Sommens J A,Westrum E F.J Chem Thermodynamics,1976;8:1115
4 Sommens J A,Westrum E F.J Chem Thermodynamics,1977;9:1
5 Kubachewski O,Alocock C B.Metallurgical Thermochemstry 5th ed,Pergamon Press,1979;181-274
6 温元凯,邵俊,王三山,陈德炜,金属学报,1979;15:98
7 Schwitzgebel K,Lowell P S,Parsons T B.J Chem Eng Data,1971;16:418
8 刘征先,郑龙如,陈念贻,阎立诚。金属学报,1981;17:65
No related articles found!
No Suggested Reading articles found!