Please wait a minute...
Acta Metall Sin  1987, Vol. 23 Issue (1): 63-69    DOI:
Current Issue | Archive | Adv Search |
ANOMALOUS THERMAL RESISTIVITY OF Au-Pd-Cr ALLOYS
HE Huachun (Institute of Precious Metals Research;Kuming)
Cite this article: 

HE Huachun (Institute of Precious Metals Research;Kuming). ANOMALOUS THERMAL RESISTIVITY OF Au-Pd-Cr ALLOYS. Acta Metall Sin, 1987, 23(1): 63-69.

Download:  PDF(594KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effect of various regimes of heat treatment on the resistance and ther- moelectromotive force of AuPd_(38.6)Cr_3 and AuPb_(36.6)Cr_8 alloys as well as the rela- tionship between their properties and structure have been investigated.The room temperature resistivity of these alloy specimens after annealing at different tem- peratures increases and maximizes at 450 and 850℃,but decreases with cold wor- king.As the cold worked specimen aged at 400 and 480℃ two peaks were ob- served on the resistivity plot and X-ray relative intensities vs time curve,while two plateaus were found on the thermoelectromotive force curve.All the pheno- mena appear correspondingly on the time axis.It seems that this anomalous behaviour is closely related to the special clusters forming in the super-saturated solid solution.
Received:  18 January 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I1/63

1 何华春.金属学报,1981;17:97
2 Mott N F.J Inst Met,1937;60:267
No related articles found!
No Suggested Reading articles found!