THERMODYNAMIC CALCULATION OF M_S AND DRIVING FORCE FOR MARTENSITIC TRANSFORMATION IN Fe-Mn-C ALLOYS
ZHANG Hongbing NI Lemin (Shanghai Technical College of Metallurgy);XU Zuyao (T.Y.Hsu)(Shanghai Jiaotong University)
Cite this article: 

ZHANG Hongbing NI Lemin (Shanghai Technical College of Metallurgy);XU Zuyao (T.Y.Hsu)(Shanghai Jiaotong University). THERMODYNAMIC CALCULATION OF M_S AND DRIVING FORCE FOR MARTENSITIC TRANSFORMATION IN Fe-Mn-C ALLOYS. Acta Metall Sin, 1987, 23(1): 42-49.

Download:  PDF(631KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The M_s temperatures of Fe-Mn-C alloys have been calculated by the appli- cation of LFG model of △G~(γ→α) with Mogutnov's △G_(Fe)~(γ→α),Hsu-A model with Orr-Chipman's △_(Fe)G~(γ→α) and Hsu-B model with Orr-Chipman's △G_(Fe)~(γ→α) and are in good agreement with the experimental values.Through the mathematical treatment, the relationship between Ms and the composition of Fe-Mn-C alloys can be ob- tained as: M_s(K)=817.4-7513.4x_C-4141.9x_(Mn)-32083.5x_cx_(Mn) (LFG model with Mogutnov's △_(Fe)G~(γ→α)); M_s(K)=829.9-7580.5x_C-4166.0x_(Mn)-15727.Sx_cx_(Mn) (Hsu-A model with Orr-Chipman's △G_(Fe)~(γ→α)); M_s(K)=829.2-7276.1x_C-2915.4x_(Mn)-43825.7x_cx_(Mn) (Hsu-B model with Orr-Chipman's △G_(Fe)~(γ→α)) in which the linear correlation coefficient of these relations are larger than 0.992. Both C and Mn depress M_s linearly and the effect of C is almost two-fold stro- nger than that of Mn.Introduction of an interaction term(x_Cx_(Mn)) between alloying elements in the present treatment shows that C and Mn enhance the effect upon M_s of each other.The driving force for transformation increases monotonically with C and Mn content and there is no singularity.The ealculted M_s and the driving force largely depend on the △G~(γ→α) model and △_(Fe)G~(γ→α) values adopted.
Received:  18 January 1987     

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I1/42

1 Zener C.Trans AIME 1946;167:550
2 徐祖耀,金属学报,1980;16:426
3 Fisher J C.Trans AIME,1949;185:628
4 徐祖耀,金属学报,1979;15:329
5 Hsu T Y(Xu Zuyao),Chang Hongbing.Acta Metall,1984;32:343
6 Hsu T Y(XU Zuyao),J Mater Sci,1985;20:23
7 Nichol T,J,Judd G.Ansell G S.Metall Trans,1977;8A:1877
8 Kato T,Fukui S,Fujikura M,et al.Trans Iron Steel Inst Jpn,1976;16:673
9 徐祖耀,张鸿冰,罗守福,金属学报,1984;20:A151
10 Hsu T Y(Xu Zuyao),Chang Hongbing,Luo Shufu,J Mater Sci,1983;18:3206
11 Shifler G J,Bradley J R,Aaronson H I.Metall Trans,1978;9A:999
12 Zener C.Trans AIME,1955;203:619
13 Mon Yiwen,Hsu T Y(XuZuyao).Acta Metall,1986;34:325
14 Aaronson H I,Domain H A,Pound G M.Trans Metall Soc AIME 1966;236:768
15 Greninger A B.Trans ASM 1942;30:1
16 Kaufman L.Radcliffe S V,Cohen M.In:Zackey V F,Aaronson H I.eds.,Decomposition of Austenite by Diffusional Processes.Interscience Publ,1962;313
17 Andrew K W.J Iron Steel Inst,1965;203:721
18 Kung C Y,Ratmet J J.Metall Trans,1982;13A:328
19 徐祖耀,马氏体相变与马氏体,科学出版社,1981,237
20 Lobo J A,Geiger G H.Metall Trans,1976;7A:1359
21 Wada T,Wada H,Elliott J F et al.Metall Trans 1972;3:1657
22 Hultgren R,Desai P.D,Hawkins D T et al.Selected Values of Thermodynamic Properties of the Elements,Ohio:ASM,1973,171
23 Breedis J F,Kaufman L.Metall Trans,1971;2:2359
24 徐祖耀,金属学报,1980;16:420
No related articles found!
No Suggested Reading articles found!