THERMODYNAMICS OF BAINITIC TRANSFORMATION IN Fe-C ALLOYS(LFG MODEL)
XU Zuyao (T.Y.Hsu)MOU Yiwen (Shanghai Jiaotong University)
Cite this article: 

XU Zuyao (T.Y.Hsu)MOU Yiwen (Shanghai Jiaotong University). THERMODYNAMICS OF BAINITIC TRANSFORMATION IN Fe-C ALLOYS(LFG MODEL). Acta Metall Sin, 1987, 23(1): 33-41.

Download:  PDF(665KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The calculated results obtained from the refined LFG model is similar to that from KRC,but there exists divergency between them in alloys with higher C contents.It seems that for treating interstitial solid solution,LFG model is more suitable over the KRC.Both the results from the two models show that △G~(γ→α+Fe_3c) is the largest,followed by △G~(γ→α+γ_1) and △G~(α-γ′) is the smallest and △G_N~(γ→α′)is far less than △G_N~(γ→α+γ_1′).At B_s,from LFG,for x_γ=0.001-0.002,△G_N~(γ→α+γ_1)△G_N~(γ→α+γ_1)- -196--237 J.mol~(-1);for x_γ=0.035,the sum of △G~(γ→α′) and △G~(α′→α″+Fe_3)is only—181 J.mol~(-1).The present work verifies again that at least at upper tem- perature range,the formation of bainite with shear mechanism is thermodynam- ically impossible.Calculation of the driving force for nucleaction(growth)gives an evidencs that the leading phase of the eutectoid reaction in hypoeutectoid steels is ferrite while that in hypereutectoid steels is cementite.
Received:  18 January 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I1/33

1 Hsu TY(Xu Zuyao),Mou Yiwen.In:Marder AR,Goldstein J I,eds.Proc,on Phase Transformations in Ferrous Alloys,TMS-AIME,1984,327
2 Hsu TY(Xu Zuyao),Mou Yiwen.Acta Metall,1984;32:1469
3 徐祖耀,牟翊文,金属学报,1985;21:A102
4 Mou Yiwen,Hsu T Y(Xu Zuyao).Acta Metall,1986;34:325
5 Fowler R H.Proc Cambridge Phil Soc,1936;32:144
6 Lacher J R.Proc Cambridge Phil Soc,1937;33:518
7 Fowler R H,Guggenheim E A.In:Statistical Thermodynamics.Cambridge University Press,1956,426-442.
8 Aaronson H I,Domain H A,Pound G M.Trans Metall Soc AIME,1966;236:753
9 Shiflet G J,Bradley J.R,Aaronson H I.Metall Trans,1978;9A:999
10 Bhadeshia H K D H.Met Sci,1981;15:178
11 Bhadeshia H K D H.Acta Metall,1980;28:1103
12 Hsu TY(Xu Zuyao),Chang Hongbing.Acta Metall,1984;32:343
13 Kaufman L,Clougherty E V,Weiss R J.Acta Metall,1963;11:323
14 Orr R L,Chipman J.Trans Metall Soc AIME,1967;239:630
15 1972;109-113
16 Kanfman L,Radcliffe S V,Cohen M.In:Zackey V F,Aaronson H I,edso,New York:Interscience,1962;313
17 徐祖耀,马氏体相变与马氏体,科学出版社,1980,258
18 徐祖耀,金属材料热力学,科学出版社,1980;279
19 Hsu T Y(Xu Zuyao).J Mater Sci,1985;20:23
20 Steven W,Haynes A G.J Iorn Steel Inst,1956;183:349[
No related articles found!
No Suggested Reading articles found!