PHASE DIAGRAM OF CU-Fe-Sn TERNARY SYSTEM |
ZHOU Huaiying ZHENG Jianxuan (Guangxi University;Nanning) |
|
Cite this article:
ZHOU Huaiying ZHENG Jianxuan (Guangxi University;Nanning). PHASE DIAGRAM OF CU-Fe-Sn TERNARY SYSTEM. Acta Metall Sin, 1987, 23(1): 141-143.
|
Abstract Isothermal sections of the phase diagram of the ternary Cu-Fe-Sn system at room temper- ature and 600℃ have been determined by X-ray powder diffraction method,microscopic observation and DTA.Eight single-phase regions:α,β,σ,ε,η,τ,ρ and θ;fourteen two- phase regions:β+η,β+θ,θ+η,θ+ρ,ρ+η,η+ε,ε+τ,τ+ρ,ρ+ε,ρ+α,α+τ,α+ε,ε+σ and α+σ:seven three-phase regions:β+η+θ,θ+η+ρ,ρ+η+ε,ρ+ε+τ,ρ+τ+α,α+τ+ε and α+σ+ε are observed at room temperature.Eight single-phase regions:α,σ,L,ρ′,τ,γ,ξ and ε; fourteen two-phase regions:L+ρ',L+ε,ρ'+ε,ρ'+τ ρ'+α,τ+ε,τ+ξ,τ+γ,ε+ξ,ξ+γ,γ+α,σ+α, γ+σ and τ+α;seven three-phase regions:L+ρ'+ε,ρ'+τ+ε,ρ'+τ+α,ε+τ+ξ,τ+ξ+γ,α+τ+γ and α+γ+σ are observed at 600℃.
|
Received: 18 January 1987
|
1 Hansen M,Anderko K,Constitution of Binary Alloys,New York:McGraw-Hill.1958;580. 633. 718 2 Smithells C J.Metals Reference Book 5th ed,London & Boston,1976. 593 616 3 陈荣贞,郑建宣,物理学报, 1983;32:933 4 Donnay J D H.Ondik H M.Crystal Data Determinative Tables,Vol.2 3rd ed,Publ.Jointly by U S DC NBS.197 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|